Basic Material Science for Plastics Laser Marking

Advancements in direct laser marking of plastics yield unprecedented marking quality, contrast, and speed. With proper application, laser marking can provide numerous manufacturing advantages and bring value to a product’s appearance and function. The newest generation of plastics material science and laser equipment systems is driving strong industry demand for indelible laser marking as an alternative to conventional ink printing. This article presents basic concepts and information relative to chemical reactions between polymers, laser additives, and specific wavelengths of laser light (emitted from various laser sources).

Practitioners often assume that laser material additives are required for all plastics laser marking applications. However, depending on the type of plastic to be laser marked and its end-use requirements for contrast and sharp/fine-line quality detail, it may not always be necessary to utilise laser-optimised material formulations. Instead, proper selection of the wavelength and type of laser will achieve the requisite degree of markability. The results will be determined by factors such as a) specific grade and properties of the resin; b) type of laser (wavelength, beam quality output mode, optical configuration, power density, peak/average power, marking speed); c) colourant and filler components; d) gloss and surface texture; and e) regrind content. Colourant compounds such as TiO2 and Carbon Black possess some degree of absorption properties at particular wavelengths. Particle size and jetness of these compounds also are factors. Further, specific resin grades, even within the same generic family, can produce very different results, e.g., Styrenics.

On the other hand, an often overlooked benefit when considering whether to incorporate laser additives is that optimised laser formulations can improve marking speed, not only the contrast and quality of the decorative or functional marking. The use of laser additives almost always decreases marking cycle times, and enables lower laser power to be used. These factors ultimately save money and increase manufacturing production.

Achieving an optimal material science chemistry formulation for plastics laser marking requires expertise in polymers, property grades within polymeric families, colourants, pigments and dyes relative to solubility, particle sizes, threshold concentration limits, colourmatch in use with laser additives, and regulatory certifications (GRAS, FDA Direct/Indirect Food Contact). Material science solutions must be cost effective, easy-to-use, and possess no deleterious effects on the polymer products? physical and chemical properties. It is thus absolutely necessary that chemists/formulators have extensive knowledge in a wide variety of laser technologies to ensure robust marking at fast manufacturing production speed.

This article focuses on beam-steered style lasers operating in the range of 1060 to 1070 nm. This includes Nd:YAG (arc lamp and diode pumped), Vanadate, and Fibre lasers. Traditional ?YAG? lasers are most popular in the laser marking industry due to their emission wavelength, power performance, and vast versatility over the past several decades. Vanadate and Fibre lasers are much newer technologies and often times their selection for use is more application specific. However, they can offer excellent results in the proper applications.

The basic mechanism of beam-steered laser marking, using a wavelength of 1060 to 1070 nm, is to irradiate the polymer with a high-energy radiation source (the laser). The radiant energy is absorbed locally by the material and converted to thermal energy. The thermal energy, in turn, induces reactions in the material. Several types of reactions are possible using this near-IR wavelength region, including at least 1) charring; 2) ablation; and 3) chemical change. Depending upon the desired marking contrast results, vastly different chemistries and laser system parameters can be selected to achieve the preferred type of reaction. Contrary to popular belief, a single laser additive that solves all marking problems does not exist!

A charring reaction occurs when the energy absorbed raises the local temperature of the material surrounding the absorption site to a sufficiently high level that thermal degradation of the polymer is caused. In the presence of oxygen this results in burning of the polymer, but within the work piece a limited oxygen supply causes a charring of the polymer to form a black mark. The darkness of the mark is dependent on the energy absorbed, as well as the material’s thermal degradation pathway.

Ablation occurs when the polymer is heated sufficiently to cause degradation and evaporation of the degradation by-products, resulting in an etched area. This marking type normally results in low contrast marks. As reference, the continuous wave (CW) CO2 lasers operate at a wavelength of 10.6 µm (far infrared spectrum). CW CO2 lasers generate comparatively much lower peak power and normally cannot produce high contrast markings on most plastics.

Chemical change, through use of additives that release steam during degradation, results in foaming of the polymer. During the foaming process, the laser energy is absorbed by an additive that is in close proximity to the foaming agent. The heat from the absorber causes the foaming agent to degrade releasing steam. Examples of foaming agents are aluminium hydroxide or various carbonates. To prevent charring, the mechanism requires the polymer to degrade at a temperature higher than that of the foaming additive. Through tight control of the laser operating parameters, quality light marks can be generated on dark substrates. Poor laser control can result in generation of a friable or low contrast mark.

Yet another method of laser marking is to use the near-IR laser energy to heat/degrade one colourant in a colourant mixture, thus causing a colour change. An example is a mixture of carbon black and a stable inorganic colourant. When heated, the carbon black is removed and the inorganic colourant is left behind. These mixed colourant systems are dependent on specific colourant stabilities and not all colour changes are possible.

In conclusion, it is important to recognise that all beam-steered lasers are not created equal. Material science chemistry alone cannot resolve all marking quality problems. The hardware and software components a laser manufacturer incorporates into its equipment make significant differences in marking quality, speed, and versatility. When procuring laser equipment, it is important to note there is not a single universal solution. Each application is unique relative to the plastic resin substrate composition and colour, and the desired marking contrast (?Dark-on-Light?, ?Light-on-Dark?, or ?Custom Colour?). Today’s modern advancements in polymeric material science and laser waveguides are quantum leaps ahead of what was not considered possible just a few short years ago.

Key Takeaways

  • Marking is a chemical reaction between the polymer, any laser additive, and the specific wavelength of the laser source.
  • Additives are not always required — a common assumption worth testing per material rather than accepting.
  • Laser marking is an alternative to conventional ink printing, and the material science is what makes it viable.
  • Wavelength must be matched to the material, not chosen by equipment availability.
  • Applied properly, marking adds value to appearance and function, not just identification.

Frequently Asked Questions

Do all plastics need a laser additive to be marked?

No, and it is a common assumption worth checking. Practitioners often assume additives are always required, but whether one is needed depends on the polymer, its colourants and fillers, and the wavelength of the laser source being used.

What actually creates the mark?

A chemical reaction between the polymer, any laser additives present, and the specific wavelength of laser light emitted by the source. Understanding that interaction is what lets you predict whether a given material and laser combination will produce a usable mark.

Why is laser marking replacing conventional ink printing?

Because the newest generation of plastics material science and laser equipment produces unprecedented marking quality, contrast and speed, with no consumable inks or solvents. Applied properly it brings manufacturing advantages and adds value to a product’s appearance and function.

Does the laser source type change the outcome?

Yes. Different laser sources emit different wavelengths, and the chemical reactions between polymers, additives and laser light are wavelength specific. Selecting the source is therefore a material science decision, not just an equipment one.

Where should a laser marking project start?

With the material. Establishing how the specific polymer grade, its colourants and additives respond to the candidate wavelengths determines everything downstream — whether additives are needed, what contrast is achievable, and what speed is realistic.

Scott R. Sabreen is founder and president of The Sabreen Group, Inc., an engineering company specialising in secondary plastics manufacturing processes – laser marking, surface pretreatments, bonding decorating and finishing and product security. Sabreen has been developing pioneering technologies and solving manufacturing problems for over 30 years. He can be contacted at 972.820.6777 or by visiting www.sabreen.com or www.plasticslasermarking.com.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴