Laser marking and engraving on PPS (polyphenylene sulfide) presents significant difficulties due to its resistance to high temperatures when subjected to laser heat. Recent advancements in colourant technology, including laser-specific carbon blacks and fibre lasers, allow for high-contrast, light-coloured, scratch-resistant marking of black glass-filled PPS, with Yellow Card certification. This innovation allows for the marking and micro-marking of data matrices, barcodes, QR codes, and unique part identification across multiple industries in India and worldwide, such as automotive, aerospace/NASA MIL electronics, emission control systems, pumps and valves, appliances, tanks, and more. The configuration and optical components of ytterbium fibre lasers require precision to ensure the production of durable, scratch-resistant, high contrast markings.

Optimal laser marking process for PPS. To create scratch-resistant, high-contrast, light-coloured markings on black glass-filled PPS, MOPA Ytterbium fibre lasers excel because they can precisely control pulse width and focused power density. This degree of precision allows for enhanced control over the surface chemical foaming process within the near-infrared wavelength range of 1060-1070nm. The optimal pulse duration ranges from 20 to 40 nanoseconds, accompanied by a pulse frequency exceeding 100 kilohertz. A precise laser configuration is essential for controlling the surface temperature, including rise and fall times; failure in achieving this may lead to the marking being easily scratched off.

Achieving high-quality laser marking on glass-filled polymers, such as PPS, necessitates the implementation of robust injection moulding techniques and the effective dispersion and distribution of laser-optimised colourants and precompounded materials. The incorporation of glass fibres can negatively affect moulding processes, subsequently influencing the quality of laser marking. Surfaces with a high resin content are critical for achieving durable marking. Surfaces with high concentration of glass fibre will produce suboptimal marking results.

Industrial Laser Marking Experts

Single-Source Total Solutions for Plastics Laser Marking – Material Science through Custom Systems Integration.

Technical Services

  • Custom laser colour match formulations & compounds, regulatory compliance, prototype samples–masterbatch, pre-compounded materials (pre-colour), laser laminates.
  • Laser equipment systems design, turnkey systems integration & training, machine vision, custom HMI, process documentation.
  • On-site problem-solving (any global location), laser process analysis & system optimisation, custom vectorised artwork.
  • Laser safety certification, complete application including design & CDRH Class 1 enclosure, laser safety officer (LSO) for internal audits.
  • Plastics injection moulding & analytical analysis, mould flow, additive-colourant dispersion/distribution.
  • Job shop marking services

The Importance of Laser Marking of Glass-Filled Polymers – The Importance of Injection Moulding Operations . To improve the structural performance of standard plastics, the incorporation of glass fibres is used. The materials that are utilised in the production of fibreglass include silica, limestone, and soda ash. “Glass emergence” is a significant surface defect frequently encountered in fibreglass-filled injection moulded products. The exposure of glass fibres leads to a surface that is rich in glass fibres. During the process of plastic melt filling and moulding, excess glass accumulates on the surface. Following the mechanisms of condensation and moulding, white marks are observed on the surface. The surfaces of moulded parts must be characterised as “resin-rich” to achieve high-quality marking, as the energy from the laser interacts with the polymer matrix. In contrast, surfaces with a high glass fibre content exhibit poor marking characteristics, and this problem exacerbates as the fibre content increases. Fibreglass exhibits limited absorption characteristics for near-infrared (NIR) laser light.

The Importance of Laser Marking of Glass-Filled Polymers – The Importance of Injection Moulding Operations

Decorative and functional markings produced by the laser must be completely readable, such as component identification, schematics, data matrix & barcode. The quality of the marking depends on the polymer, additives and colourants, injection moulding processes, and the laser source. Moulded polymer surface problems which inhibit readability can affect safety, performance and function of the product.

What is Polyphenylene Sulfide (PPS)?

Polyphenylene Sulfide (PPS) is a high-temperature, semi-crystalline engineering thermoplastic. Within the industry, PPS is known as THE plastic that performs like metal. The properties of PPS, similar to other high-temperature performance plastics including PEEK and LCP, depend on its crystallisation behaviour. Two distinct forms of PPS are sold: “Branched” molecular structure and “Linear”. Among the most recognisable brands are Celanese Fortron® Solvay Ryton®, SABIC Supec, Toray Torelina, and DIC PPS. The branched version tends to be more rigid. The linear usually offers better mechanical and flexural strength, as well as higher melt stability. Linear PPS also has fewer ionic impurities. Glass-filled fibres (30 percent and 40 percent) and glass fibre/mineral mixtures to standard PPS allow for specialised and demanding applications. Electronics manufacturers commonly select 40 percent glass-filled PPS for insulation and connector products.

Celanese Fortron®

Frequently Asked Questions About Laser Marking PPS

What is Polyphenylene Sulfide PPS?Polyphenylene Sulfide (PPS) is an engineering thermoplastic known for its high-temperature, semi-crystalline properties. In the plastics industry, PPS has become known as the plastic that delivers performance akin to metal. The characteristics of PPS, similar to other high-performance plastics that withstand high temperatures such as PEEK and LCP, are influenced by its crystallisation behaviour. There are two unique types available: Branched” molecular structure and “Linear”. Some of the most well-known brands include Celanese Fortron® Solvay Ryton®, SABIC Supec, Toray Torelina, and DIC PPS. The branched version tends to be more rigid. The linear usually offers better mechanical and flexural strength, as well as higher melt stability. Linear PPS also has fewer ionic impurities. Glass-filled fibres (30 percent and 40 percent) and glass fibre/mineral mixtures to standard PPS allow for specialised and demanding applications. Electronics manufacturers commonly select 40 percent glass-filled PPS for insulation and connector products.

Is it possible to achieve light-coloured laser marking contrast on black PPS? Yes, new advancements in colourant technology, including laser-specific carbon blacks and fibre lasers, allow for high-contrast, light-coloured, scratch-resistant marking of black glass-filled PPS, with Yellow Card certification. This advancement allows for the marking of data matrices, barcodes, QR codes, and unique part identification.

What is the best type of laser for marking PPS? MOPA fibre lasers for marking plastics are ideal because they can precisely control pulse width and power density. This precision allows for enhanced control over the surface chemical foaming process. Precise laser configuration is important for controlling the surface temperature.

MOPA fibre lasers for marking plastics

laser marking pps examples

How Do Laser Additives Work?

laser pps marking mechanisms

Does Fibreglass Affect Laser Marking?

Yes, fibreglass affects laser marking. Materials used to make fibreglass are silica, limestone and soda ash. Silica is the main material used to form the glass while soda ash and limestone are used to lower the melting temperature. “Glass emergence” is a serious surface defect that commonly affects fibreglass-filled injection moulded products. The exposure of glass fibres causes a glass fibre-rich surface. Excess glass forms on the surface during plastic melt filling and moulding. After condensation and moulding, white marks appear on the surface. Moulded part surfaces must be “resin-rich” in order to produce high quality marking, whereby the energy from the laser interacts with the polymer matrix. Conversely, glass fibre-rich surfaces mark poorly, and the issue gets worse with higher fibre content. Fibreglass itself is not a good absorber of near-IR (NIR) laser light.

ABS injection moulded writing pens

Glass Emergence defect on 25% glass-filled polyamide. Courtesy Topworks Plastic Mould

For high-quality marking, homogenous distribution/dispersion of colourants and additives is just as crucial as resin-rich surfaces. To determine if distribution/dispersion issues are present, it is recommended to setup the laser to mark/scan continuously across the entire part surface. The result shows (left to right) moulded pen displaying excellent gold-on-black chroma marking (left), middle two pictures showing poor chroma distribution and far-right showing excellent uniform distribution.

Glass Emergence defect on 25% glass-filled polyamide. Courtesy Topworks Plastic Mould

ABS injection moulded writing pens

What is Polyphenylene Sulfide PPS Plastic?

Polyphenylene Sulfide (PPS) is a high-temperature, semi-crystalline engineering thermoplastic. Within the industry, PPS is known as THE plastic that performs like metal. The properties of PPS, similar to other high-temperature performance plastics including PEEK and LCP, depend on its crystallisation behaviour. Two distinct forms of PPS are sold:

“Branched” molecular structure and “Linear”. Among the most recognisable brands are Celanese Fortron® Solvay Ryton®, SABIC Supec, Toray Torelina, and DIC PPS. The branched version tends to be more rigid. The linear usually offers better mechanical and flexural strength, as well as higher melt stability. Linear PPS also has fewer ionic impurities. Glass-filled fibres (30 percent and 40 percent) and glass fibre/mineral mixtures to standard PPS allow for specialised and demanding applications. To achieve a fully crystalline state, mould temperatures of at least 275 to 300 degrees Fahrenheit are required.

When PPS is moulded below 275 degrees Fahrenheit, the mouldings are amorphous, or semi crystalline, and remain in this state until they are exposed to higher service temperatures. If the service temperature exceeds the moulding temperature, the parts will become more crystalline, resulting in dimensional and property changes.

To achieve a fully crystalline state, mould temperatures of at least 275 to 300 degrees Fahrenheit are required. When PPS is moulded below 275 degrees Fahrenheit, the mouldings are amorphous, or semi crystalline, and remain in this state until they are exposed to higher service temperatures. If the service temperature exceeds the moulding temperature, the parts will become more crystalline, resulting in dimensional and property changes.

Laser Marking PPS Technical Articles

laser application by sabreen

Laser Marking PPS With Laser Additives

Laser Marking Glass-filled Plastics

Laser Marking Glass-filled Plastics

Fibre Lasers for Marking Plastics

Fibre Lasers for Marking Plastics

Laser Marking Additives for Plastics

Laser Marking Additives for Plastics

Laser Additives Enhance Laser Marking

Laser Additives Enhance Laser Marking

Inline Plastics Laser Marking

Inline Plastics Laser Marking

laser marking pps article

Laser Marking PPS Technologies


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴