FDA-Approved Additives Boost Inline Plastics Laser Marking

FDA-Approved Additives Boost Inline Plastics Laser Marking

Fast speed, superior contrast and cost-savings are among the significant benefits of incorporating novel FDA-approved additives into polymers for laser marking. Chemical additive breakthroughs produce jet black and light-coloured contrast on moulded and extruded products, both “on-the-fly” and during secondary operations. Designed for affordable fibre lasers, inline inkless laser marking now replaces rotary gravure and pad printing.

Product applications Many clear, semi-transparent and opaque coloured polymers, including nylons, PET, polycarbonates, polyolefins, PVC, styrenics, TPU/TPE (for wearables) are uniquely formulated using non-heavy metal, FDA-/EFSA- (European Food Safety Authority) approved additives to achieve high-contrast marking quality. Polymer clarity, spectral transmission and base physical properties are not affected. Non-contact, digital laser marking replaces expensive adhesive labels and ink-chemical printing processes. The result is a cost-effective, environmentally friendly, superior aesthetic appeal in the application.

“On-the-fly” laser marking is performed on moulded and extruded products, such as wire/cable, tubes and pipes.

Key Takeaways

  • Three surface reactions create the mark — carbonisation (charring), foaming, and colourant colour change.
  • Loading runs 0.01–4.0% by weight in the final part, selected by polymer, substrate colour, target contrast and certification needs.
  • Additives are 15% or more faster than non-optimised formulations, and replace rotary gravure and pad printing outright.
  • Dispersion problems, not dosing errors, are the usual cause of low additive content in finished parts — raise back pressure and screw speed.
  • 21 CFR 178.3297 conditions A–H cover FDA food-contact approval; ISO 10993 qualification extends to medical device biocompatibility.

Marking speeds for polyolefin synthetic wine corks and undercap promotions on linerless beverage closures are capable of 2,000 pieces per minute for alphanumeric text and graphics. Marking speed is a function of many variables, including polymer type, substrate colour, laser additive type and loading level, cable size (weight), laser type and power, software, number of alphanumeric characters, text height, length of text string, space between characters, bar code/ data matrix, logos/graphics, single-stroke or true-type filled fonts, fill direction and continuous or repeating text. Use of the proper formulated additive-colourant will ensure that “power density” at the mark surface is not the limiting factor. Rather, the beam-steered galvanometers will be operating at maximum speed.

Due to the complexity of factors influencing on-the-fly production marking capability, every application must be precisely examined. There are few, if any, rules that can be extrapolated. However, for general purposes, consider the following nylon polymer example: 50-watt fibre laser, 254mm flat field lens, 100 alphanumeric characters, 2mm height, comprising a repeating text string length of 14.68 inches with a marking time of 0.232 seconds. The calculated speed is approximately 315 linear-feet per minute.

Frequently Asked Questions

Which polymers can be marked with FDA-approved laser additives?

Clear, semi-transparent and opaque coloured polymers including nylons, PET, polycarbonates, polyolefins, PVC, styrenics and TPU/TPE for wearables. Polymer clarity, spectral transmission and base physical properties are not affected.

My finished parts contain less additive than calculated. Why?

Almost always non-uniform distribution during extrusion or moulding rather than a dosing error. Increasing back pressure and screw rotation speed resolves most cases. Precompounded material outperforms colour concentrate for uniformity, and hand-mixing should be avoided entirely.

What are the three laser marking reaction mechanisms?

Carbonisation or charring, where absorbed energy thermally degrades the polymer to produce dark marks. Foaming, where an additive releases steam during degradation to create durable light marks on dark substrates. And colour change, where laser energy degrades one colourant in a mixture — for example removing carbon black to leave a stable inorganic colourant behind.

How fast can inline marking run in practice?

Marking speeds for polyolefin synthetic wine corks and undercap promotions on linerless beverage closures reach 2,000 pieces per minute. A worked nylon example — 50 W fibre laser, 254 mm flat field lens, 100 characters at 2 mm height, 14.68 inch repeating string, 0.232 s marking time — calculates to roughly 315 linear feet per minute.

Why do light-coloured foamed marks sometimes scratch off?

Poor laser control. The foaming mechanism requires tight parameter control so the polymer degrades at a higher temperature than the foaming additive. Without it, the mark is friable or low contrast and has poor durability.

Polymeric Laser Marking Reaction Mechanisms

The advancements achieved in formulating laser additives for use with near infrared lasers (1060-1080nm wavelength) are their compatibility with Ytterbium fibre, Vanadate and predecessor Nd:YAG lasers. Most polymers do not possess near infrared absorption properties without chemical additives. Polymers that can be marked by lasers are those that absorb laser light and convert it from light energy to thermal energy. Experts utilise additives, fillers, pigments and dyes to enhance the absorption of laser energy for localised colour changes. Vastly different formulation chemistries and laser optics/setup parameters are used, depending upon the desired marking contrast and functionality.

The most common surface reaction mechanism is termed thermal chemical “carbonisation” or “charring,” whereby the energy absorbed in the substrate raises the local temperature of the material surrounding the absorption site high enough to cause thermal degradation of the polymer. The darkness or lightness of the mark is dependent on the energy absorbed, as well as the material’s unique thermal degradation pathway. By optimising the laser setup, there will be minimal surface carbonisation residue.

A second surface reaction is chemical change through use of additives that release steam during degradation, resulting in foaming of the polymer. During the foaming process, the laser energy is absorbed by an additive that is in close proximity to the foaming agent. The heat from the absorber causes the foaming agent to degrade, releasing steam. Through tight control of the laser-operating parameters, high-quality and durable light marks can be generated on dark substrates. Poor laser control can result in generation of a friable or low-contrast mark, which easily can be scratched (poor durability).

Third, laser energy is used to heat/degrade one colourant in a colourant mixture, resulting in a colour change. An example is a mixture of carbon black and a stable inorganic colourant. When heated, the carbon black is removed, leaving behind the inorganic colourant. These mixed colourant systems are dependent on specific colourant stabilities and not all colour changes are possible.

Laser Additives

Laser additives improve the degree of contrast, which can be further intensified by changing the laser setup parameters. Polymers possess inherent characteristics to yield “dark-coloured” or “light-coloured” marking contrast. Some colourant compounds containing low amounts of Titanium dioxide (TiO2 ) and carbon black also may absorb laser light and, in some instances, improve the marking contrast. Each polymer grade, even within the same polymeric family, can produce different results. Additive formulations cannot be toxic or adversely affect the products appearance, physical or functional properties.

Compared to ink printing processes (pad/screen printing and inkjet), laser additives are cost-saving and demonstrate 15-percent (or greater) faster marking speeds versus non-optimised material formulations. Laser additives are supplied in pellet granulate and powder form. Granulate products can be blended directly with the polymer resin, while powder forms are converted to masterbatch. Most easily are dispersed in polymers. Based upon the additive and polymer, the loading concentration level by weight (in the final part) ranges from 0.01 percent to 4.0 percent.

Both granulate and powder form can be blended into precompounded colour material or colour concentrate. The selection of which additive to incorporate depends upon the polymer composition, substrate colour, desired marking contrast colour and end use certification requirements. Some additives contain mixtures of antimony-doped tin oxide and antimony trioxide that can impart a “grayish” tint to the natural (uncoloured) substrate opacity. Other additives can contain aluminium particles, mixed metal oxides and proprietary compounds. Colour adjustments are made using pigments and dyes to achieve the final colourmatch appearance. As commercially supplied, specific additives (also used for laser welding) have received FDA approval for food contact and food packaging use under conditions A-H of 21 CFR 178.3297 Colourant for Polymers. For the European Union, there are similar compliance statements. Certification conditions are specific for polymer type, loading level threshold and direct or indirect contact. Further qualification of FDA-approved additives blended into a “final part” can achieve biocompatibility of medical devices (reference International Standard ISO-10993).

Processing Considerations

During the laser additive loading/colourmatch chemistry, it is not uncommon for a finished product to contain less laser additive than the calculated amount. This problem almost always relates to non-uniform distribution during extrusion or moulding. Simple adjustments to the moulding machine, such as increasing the back pressure and screw rotation speed, will resolve most issues. Homogeneous distribution/dispersion of laser additives throughout each part is critical to achieve optimal marking performance. For extrusion, injection moulding and thermoforming operations, precolour compounded materials versus colour concentrate yields better uniformity. Hand-mixing should be avoided. Mould flow and gate type/location are important factors.

Laser Technology

The advancements in laser technology have been instrumental to the rapid development of the newest generation of FDA-approved laser additives. The emergence of nanosecond Ytterbium Fibre lasers is one of the most significant advancements for marking, welding and cutting. Fundamentally, fibre lasers are different than other solid state marking lasers. With fibre lasers, the active medium that generates the laser beam is dispersed within a specialised fibre optic cable. In contrast to fibre-delivered lasers, the entire path of the beam is within fibre optic cable all the way to the beam delivery optics.

Fibre lasers yield superior beam quality and brightness compared to Nd:YAG lasers. One metric for beam quality is M2. The smaller the M2 value, the better the beam quality, whereas M2 = 1 is the ideal Gaussian laser beam. A laser with superior beam quality can be focused to a small spot size, which leads to high energy density. Fixed and variable pulse (MOPA) fibre lasers with pulse energy up to 1 mJ and high power density can mark many historically difficult polymers. Vanadate lasers also possess a small M2 value with shorter pulse width than fixed fibre and YAG lasers. Pulse duration influences the degree of heat and carbonisation into the material. Short(er) pulse width can be advantageous for sensitive polymeric applications.

IPG Photonics, a leading developer and manufacturer of high performance fibre lasers, offers both fixed pulse (sometimes referred to as “Q-switch”) and variable short pulse (MOPA) lasers. Application development is highly specific. The selection of which laser type to integrate is determined by the output characteristics of the laser interacting with the optimised polymer material. Reference the graphs below, representing Temporal Pulse Shapes of Fixed and Variable (MOPA) Pulse Length Ytterbium Fibre Lasers – IPG Photonics.

Ytterbium Fibre Lasers

When setting up a fixed pulse length fibre laser for marking, two inputs must be set.

  • Pulse repetition rate (often referred to as pulse frequency)
  • Pump power in percent (100 percent refers to the maximum possible electrical input to the pump diodes)

When setting up a variable short pulse MOPA fibre laser for marking, three inputs are set.

  • Pulse duration (often referred to as pulse length)
  • Pulse repetition rate (pulse frequency)
  • Pump power in percent (100 percent refers to the maximum possible electrical input to pump diodes)

For both graphs on the previous page, the particular combination of parameter inputs controls the output properties of the laser beam, namely the pulse energy, the peak power (the highest instantaneous peak of the pulse energy, J/pulse duration) and the average power (average power in Watts = pulse energy in joules x pulse repetition rate in Hz).

All beam-steered Fibre, Vanadate and YAG lasers are not created equal. The hardware and software components incorporated into a laser manufacturer’s systems makes significant difference in marking contrast, quality and speed. A primary attribute is the power density (watts/cm2) at the mark surface (which is different than the raw output power of the laser). The output mode of the laser beam is critical to the marking performance. These output modes relate to factors including the beam divergence and power distribution across the diameter of the laser beam.

Power density is a function of focused laser spot size. Focused laser spot size for any given focal length lens and laser wavelength is a function of laser beam divergence, which is controlled by laser configuration, mode selecting aperture size and upcollimator (beam expander) magnification.

Pulse repetition rate and peak power density are critical parameters in forming the mark and achieving the optimal contrast and speed. The arithmetic curves of power versus pulse repetition rate are inversely proportional. High peak power at low frequency increases the surface temperature rapidly, vaporising the material while conducting minimal heat into the substrate. As the pulse repetition increases, a lower peak power produces minimal vaporisation, but conducts more heat. Additional contributing factors that influence the marking contrast and quality are, of course, beam velocity and the vector line separation distance.

Conclusion

The newest generation of FDA-approved laser additives incorporated into polymers yields superior marking contrast, line edge detail and speed. Inline, on-the-fly laser marking now replaces rotary gravure and pad printing. Advancements in affordable fibre laser technology have been instrumental. These benefits rapidly offset the incremental material additive cost. Optimised material-science chemistry for plastics laser marking requires expertise in polymers, colourants, pigments and dyes relative to solubility, particle sizes, threshold concentration limits, colour match and regulatory certifications (GRAS, FDA Direct/Indirect Food Contact). All lasers are not created equal.

Acknowledgements

  • Dr. Tony Hoult, IPG Photonics, “Laser Marking with Fibre Lasers,” Industrial Laser Solutions, September 2012.
  • BASF Corporation Mark-it™ Laser Marking Pigment Technical Bulletin 2002, with technical content contributions from The Sabreen Group, Inc.
  • Bruce Mulholland (Hoechst Technical Polymers) and Scott Sabreen (The Sabreen Group, Inc.), “Enlightened Laser Marking,” Lasers&Optronics, July 1997.
  • Daniel S. Burgess, Scott R. Sabreen, & Carl Baasel Lasertechnik GmbH, Feature Article, “Laser Marking: A Clean Economical Packaging Solution,” Photonics Spectra, November, 2001.

Scott R. Sabreen is founder and president of The Sabreen Group, Inc., an engineering company specialising in secondary plastics manufacturing processes – laser marking, surface pretreatments, bonding decorating and finishing and product security. Sabreen has been developing pioneering technologies and solving manufacturing problems for over 30 years. He can be contacted at 972.820.6777 or by visiting www.sabreen.com or www.plasticslasermarking.com.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴