Breakthrough Anti-Counterfeit Technology for Plastics Products

Abstract

The Global Brand Counterfeiting Report 2018 states the amount of total counterfeiting globally has reached $1.2 trillion in 2017 and is bound to reach $1.82 trillion by the year 2020, which includes counterfeiting of all equipment and products from military defence to consumer goods. As per the 2017 report, the amount of sale of counterfeit products through the e-commerce platform is $280 billion1. Counterfeiting threatens the global economy and public health through the production of inferior products that circumvent consumer protection regulatory channels. No single anti-counterfeit technology can effectively protect all products and circumstances. A layered approach that combines multiple features into the product and packaging works best. This tactical methodology is ideal for plastic products that have value-added decorating and finishing. This article introduces a new anti-counterfeit technology and examines three levels of authentication security for plastics products.

Key Takeaways

  • Counterfeiting reached $1.2 trillion globally in 2017, with $280 billion of it moving through e-commerce.
  • Security works in three levels — L1 overt, L2 covert, L3 forensic — and layering them is what actually works.
  • No single technology protects every product. There are still no global standardised anti-counterfeit identification criteria.
  • Nano laser marking under 25 microns is invisible to the naked eye and appears as a dotted or solid line to a scanner.
  • Taggants range from 20 to 1,200 microns, are uniquely encoded per customer, and now verify via smartphone.

Frequently Asked Questions

What are the three levels of anti-counterfeiting security?

Level 1 (overt) features are clearly visible and need no detection device. Level 2 (covert) features require specific equipment to verify and their details are not disclosed. Level 3 (forensic) covers taggants and laboratory-verifiable markers. Used in combination they provide layered protection.

How does breath or vapour authentication work?

Submicron microstructures forming an image, logo or text code are permanently etched into polymers, thin films, metals and glass. An invisible security code appears temporarily when vapour is applied by mist, then disappears within seconds as the moisture evaporates. No authentication instrument is needed.

Why is that approach useful in developing markets?

Because verification needs no tool, no app, no power and no internet connection. That makes it deployable anywhere, which matters most in regions where readers and connectivity cannot be assumed.

How small is nano laser marking, and why does size help?

Micro and nano text is less than 25 microns high, invisible to the naked eye and typically hidden in an inconspicuous area. Counterfeiters cannot replicate it without the original artwork files, and when scanned or photocopied the microprint appears merely as a dotted or solid line unless resolution is exceptionally high.

What are chemical taggants and how are they verified?

Microscopic uniquely encoded particles, typically 20 to 1,200 microns, added to moulded components without changing colour or material properties. Each acts as a virtual fingerprint. Verification uses inexpensive handheld readers, scanners or smartphones, and taggants are supplied as dry particles for compounding or as finished masterbatch.

Introduction

Authentication technologies are critical for supporting brand strategies and reducing the risk of fraud. Anti-counterfeit features enable the authentication of an item and function as a deterrent to anyone considering counterfeiting a product based on the difficulty or cost involved. The growth in counterfeit products can be attributed, in large portion, to the fact that counterfeiters employ sophisticated technology in manufacturing and packaging their fake products. Some operate entire production plants. Despite this epidemic problem, there are currently no global standardised anti-counterfeit identification criteria, and efforts to tackle counterfeits have focused primarily on making packaging difficult to imitate. It is imperative that new and more sophisticated technologies be introduced in the war against counterfeiting. One new covert optical security technology, Snowleopard, is presented below.

Anti-counterfeiting Technologies

Security features can be divided into three levels, i.e., Level 1 Security (L1S) (Overt), Level 2 Security (L2S) (Covert) and Level 3 Security (L3S) (Forensic). These three levels of security in combination provide comprehensive, layered security protection solutions. Figure 1 highlights authentication features examined in this article, i.e., optical security, security printing, security inks and chemical taggants.

Overt and covert security authentication features are effectively incorporated into layered protection. Overt techniques are clearly visible and do not require detection devices. Covert technologies typically require specific equipment to be verified, as the details of the technology are not disclosed. Most of the recent developments in overt and covert technologies have embedded hidden features to make them more difficult to be illegally replicated.

Featured Technology – Optical Security (Covert)

A new, state-of-the-art covert technology – Snowleopard – has been introduced whereby submicron microstructures “image/logo/text codes” are permanently etched into polymers, thin-films, metals and glass products. Polymer materials can be transparent, translucent or opaque (any colour). Authentication, by way of an invisible security code, temporarily appears when vapour is applied by mist and rapidly disappears in seconds as moisture evaporates (Figure 2). No authentication instruments are necessary.

This covert feature is deployed worldwide in specialised applications in which authentication is simply performed via “vapour breath,” and is ideal for companies requiring brand protection in underdeveloped countries. The technology is easily integrated as stand-alone or part of a layered defence. Submicron security codes are etched into the moulded product itself. Alternatively, codes can be etched into tamper-evident security labels.

The process is non-contact and conducted at atmospheric conditions. No inks, solvent chemicals, films, labels or lasers are involved. The delivery format is performed inline or offline. Tabletop-sized industrial equipment requires only electricity.

A second example of optical security authentication is optical variable devices (OVDs). OVDs are complex security images that exhibit various optical effects depending on the amount of light striking the OVD and the angle in which the OVD is viewed. OVDs cannot be photocopied or scanned and cannot be accurately replicated or reproduced. Many features have 3D effects and colour-changing properties. OVDs, similar to holograms, generally involve image flips or transitions, colour transformations and monochromatic contrasts. The construction is typically composed of a transparent film (as the image carrier), plus a reflective backing layer, which is typically a very thin layer of aluminium or copper, to produce a feature characteristic hue.

Additional security features may be added by the process of partial de-metallisation, whereby some of the reflective layer is chemically removed to give an intricate outline to the image. The reflective layer can be so thin as to be transparent, resulting in a clear film with more of a ghost reflective image visible under certain angles of viewing and illumination.

For plastics products, a powerful layered defence strategy combines OVDs (holograms) with submicron etched codes (via Snowleopard) to create tamper-evident security labels. Submicron codes can be etched into the product and/or a feature in the OVD label. Secure adhesive labels have specific text built into the layered self-adhesive construction and, when peeled or removed, they exhibit the word “VOID” in both the removed film and the adhesive layer left behind. The text “VOID” could be replaced by customers’ brand, logo or message. Layered substrates – commonly polyester or biaxially-oriented polypropylene (BOPP) face materials – gain significance since they can be uniquely customised with infinite colour combinations and metallisation.

Security Printing Technologies: Micro Printing and Nano Laser Marking

Micro/nano printing, including laser engraving/marking, utilises single-point font sizes with ultra-high resolution designs. One example is guilloche printing, intricate and complex geometric patterns that consist of numerous interwoven fine lines (see Figure 4). Each pattern is uniquely generated, therefore exact reproduction is nearly impossible. Effects are often combined with rainbow colouring.

Security ink technologies include: UV-sensitive inks, thermochromic, photochromic, luminescent, fluorescent, iridescent, phosphorescent, etc. UV- and fluorescent-sensitive inks are available in various colours and glow under different wavelengths of UV light, while invisible to the naked eye. For example, a pad, screen or gravure printed thermochromic ink graphic/logo will change colour (discolouration reaction) simply by rubbing a finger on the printed area. Each secure ink chemistry, utilised alone or in combination, combined with security printing technologies offers powerful authentication.

Nano Laser Engraving/Marking

On-product marking by laser of micro/nano text is so small – less than 25 microns high – it is invisible to the naked eye, thus incredibly difficult for counterfeiters to replicate without the original artwork files. Microtext is frequently hidden in an inconspicuous or unnoticeable area on the product. Laser-engraved data and images are permanent and secure. When the item is placed in a photocopier or scanner, the line of microprint text will appear to the scanner as a dotted or solid line if the scanning resolution is not exceptionally high.

Additionally, laser marking produces raised lettering that can enable authentication at the touch of a finger. Camera vision systems ensure accurate placement of data. Sometimes an easily overlooked spelling error is inserted in the micro text. Microprinting can serve to confirm the fact that the product is genuine. Laser waveguide types and configurations – such as UV, CO2 and ytterbium fibre – including pico/femto, are commonly used.

Chemical, Molecular Taggant Technologies

Taggants, originally developed by 3M, can be added into moulded plastic components and finished goods. Taggants do not change the colour appearance of the plastic and can be used in any colour, including transparent plastic. A taggant is one of the strongest protective measures, as few materials can be used within products without changing material properties and functions. Multiple taggant types are available to deploy and enforce strong and viable brand protection strategies.

One of the most significant recent advancements is product authentication using smartphones. Taggants, microtaggants and nanotaggants are uniquely encoded for each customer or product. Particles are microscopic, typically ranging in size from 20 microns to 1,200 microns. Each particle is uniquely encoded, essentially serving as a virtual fingerprint. In its most basic form, the taggant is a unique numeric code sequence in a multicoloured layer format. In more complex form, it provides multiple layers of security through incorporation of several nanotaggant technologies in a single microscopic particle. Verification and detection are done with a variety of inexpensive handheld readers and scanners, including smartphones. The taggants are available in dry particle form for compounding or as a finished masterbatch. The taggants can be used in a variety of plastic resins and colours with no change in processing conditions.

Conclusion

Counterfeiting threatens the global economy and public health through the production of inferior products that circumvent consumer protection regulatory channels. In response to this threat, new state-of-the-art covert technology – whereby submicron microstructures, image/logo/text codes, are permanently etched into polymers – offers innovative security options. A layered approach that combines anti-counterfeit technologies – overt, covert and forensic (taggants) – works best. This is ideally suited for captive and custom plastics manufacturers that presently conduct value-added decorating and finishing operations, or plan to.

This article presents anti-counterfeiting methods. Note that the comments and conclusions must be viewed as general to each group of technologies, and, inevitably, there will be exceptions with, and omission of, some more special applications. Some of these technologies are trademark brands and/or protected by international patents and may be available only from licensed suppliers, subject to fees. Alternatively, some can be applied in-house with costs on materials and processing, and most are available from specialist suppliers.

Scott R. Sabreen is founder and president of The Sabreen Group, Inc., an engineering company specialising in secondary plastics manufacturing processes – product security, laser marking, surface pretreatments, bonding, decorating and finishing. Sabreen has been pioneering technologies and solving manufacturing problems for over 30 years. He can be contacted at 972.820.6777 or by visiting www.Sabreen.com. For information regarding Snowleopard, contact The Sabreen Group.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴