industrial coating of plastics is a cornerstone process for decorating, finishing, and mass customisation. Liquid coatings are highly versatile allowing for infinite functional and aesthetic possibilities Coatings add value and are cost-effective and eco-friendly. Coating processes are multifaceted and require proper engineering. The effects of paint chemistry and polymer compatibility must be understood. Surface quality and cleanliness are essential for adhesion and defect-free quality. This article is the first in a series to discuss liquid coatings for plastics. In this issue, we examine polymer properties, types of interactions between coatings and substrates, polypropylene applications, and coating technologies.

The terms “coating” and “painting” are often interchanged. Generally, the purpose of “painting” is for aesthetics while “coating” is for performance by applying a functional material layer on the substrate. Examples of performance coatings include waterproofing, self-cleaning, anti-microbial, rust & corrosion prevention, UV/weatherability protection, flexibility & elasticity, and colour retention. To achieve adhesion plastic parts must be free of static, dirt, oils, fingerprints, mould release residues, etc. Low molecular weight oxidised materials (LMWOM) such as antioxidants, plasticisers, slip, and antistatic agents, colourants/pigments, and stabilisers can change the paintability of a part, and result in delamination and other defects. Due to the hydrophobic nature of Polypropylene (PP) and many polymers plasma pretreatment is necessary, and sometimes in conjunction with chlorinated polyolefin chemical adhesion promotors.

Key Takeaways

  • Paint and polymer interact chemically, thermally and mechanically — no interaction may compromise the plastic’s properties.
  • PP is the “steel” of the plastics industry, tough, rigid, crystalline, non-polar and 100% recyclable.
  • Paintability is a design decision. Grades differ even within a polymer family, so the polymer choice sets the ceiling.
  • Three coating families — single component lacquers, two component thermosets and UV — all available in waterborne chemistries.
  • Recycled PP is a real coating market. Automotive batteries become building products warranted for 25 years or more.

Frequently Asked Questions

Why is polypropylene hard to paint?

PP is hydrophobic, non-polar and chemically inert, which means poor surface wettability. It is a linear hydrocarbon resin in the polyolefin family, and upon polymerisation forms atactic, isotactic or syndiotactic chain structures depending on methyl group position — each affecting behaviour.

What has to be considered when matching paint to plastic?

Three interaction types: chemical, thermal and mechanical. None may compromise the plastic’s properties. The complication is that there are many plastics and many grades within each family, each with different paintability, and primary processing contributes as well.

What coating technologies are available for plastic finishing?

Three main categories. Single component lacquers are easy to use with low cost per square foot and dry by solvent or water evaporation, typically in 30 minutes or less. Two component thermosets and UV coatings make up the others. All three are available in waterborne chemistries.

Can recycled polypropylene be coated successfully?

Yes, and it is a significant application. Recycled automotive batteries become building interior and exterior products, some warranted by the manufacturer for over 25 years, with coating the preferred decorating process for mass customisation.

When are single component lacquers the right choice?

Where cost per square foot and ease of use matter most and the performance requirement is moderate. They can be formulated for hardness and abrasion resistance, or made more flexible for soft plastics, and they harden entirely by evaporation at room temperature or under low bake.

Paint-Polymer Compatibility

The effects of paint chemistry and plastic compatibility need to be understood to achieve robust operations and end-use performance. The selection of paint and plastic has several interactions including chemical, thermal and mechanical2. It would not be acceptable for any element to compromise the plastic properties. Design engineers must select the optimal polymer, a balance between performance and paintability. One complexity is that there are so many different plastics and grades, even within the same polymer family, each possessing unique properties and degree of paintability. Primary processing is a contributing factor including material purity, mould temperature, gating, degassing, degree-of-crystallinity, etc.

Chemical effects – Paint solvents and chemical interactions may damage the plastic. It is often desirable for the paint solvents to attack (etch) the plastic which to a limited degree can improve adhesion bonding. However, solvents can cause surface crazing, environmental stress cracking, swelling, softening, dissolution of polymer substrate, and many solvent-related defects (e.g., pinholes, solvent pop & voids).

Thermal effects – Some types of paints require elevated temperature curing. High(er) temperatures (relative to polymer moduli) may relieve moulded-in part stresses causing warpage. Paint shrinkage during curing may produce residual stresses. Extreme temperatures may degrade the polymer. When oven curing, temperature rise should be gradual.

Mechanical effects – The strength and stiffness properties of the dry paint must be compatible with the plastic and function together as one. Selection of a paint system that is not properly matched to a given plastic substrate can lead to premature failure, i.e., “elastic mismatch”.

Polypropylenes

Polypropylene (PP) is often referred to as the “steel” of the plastic industry because of the various ways in which it can be modified for particular purposes. PP is a tough, rigid and crystalline, non-polar thermoplastic produced from propene (or propylene) monomer. 100% recyclable. PP is difficult to bond because it is hydrophobic, non-polar, chemically inert, i.e., poor surface wettability. PP has a linear hydrocarbon resin belonging to the group of polyolefins. The chemical formula of PP is (C3H6)n.

Polypropylenes

Upon polymerisation, PP can form three basic chain structures depending on the position of the methyl groups:

  • Atactic (aPP) – Irregular methyl group (CH3) arrangement
  • Isotactic (iPP) – Methyl groups (CH3) arranged on one side of the carbon chain
  • Syndiotactic (sPP) – Alternating methyl group (CH3) arrangement

There are two main types of PP: homopolymers and copolymers. The copolymers are further divided into block copolymers and random copolymers. Homopolymer PP is a general-purpose grade. Block copolymer PP has co-monomer units arranged in blocks and contains anywhere between 5% to 15% ethylene. Random copolymer PP has the co-monomer units arranged in irregular or random patterns along the molecule, typically 1% to 7% ethylene1. The melting point of PP occurs at a range which means the temperature set point for oven cure should be assessed based upon its grade.

  • Homopolymer: 160-165°C
  • Copolymer: 135-159°C

Antistat. PP has excellent electrical insulating properties and a tendency to retain static charges that attracts dirt to the surface. Antistatic additives can “bloom” to the surface dissipating electrical charges but causes paint delamination. Additionally, white film (bloom) can show on the surface of dark colours after several months.

Effects of radiation Ultraviolet (UV). PP is greatly affected by UV radiation. Exposure to direct sunlight will cause loss of strength properties, unless a UV inhibitor or high loading of carbon black pigment is used. Even with high inhibitor or pigment addition, service life expectancy under severe sunlight conditions is limited.

Polymer design considerations for PP and low surface energy polymers:

  • PP copolymers can be easier to adhere/bond than homopolymers.
  • Nylons and polycarbonates are hygroscopic and must be dried. PP is not hygroscopic, but if the resin pellets have moisture on the surface that will cause the same problems as wet hygroscopic materials.
  • Nylon “bulk” properties are hydrophobic and “surface” properties are hygroscopic1.
  • Nylon 6 absorbs moisture more readily than Nylon 66, whereby moisture acts as a plasticiser. Nylon 6 can be easier to bond than Nylon 11 or 12.
  • Acetal POM copolymers (Celcon) can be easier to bond than homopolymers (Delrin).
  • Polyethylenes are easier to bond. Ensure that PP is required.

Applications from Recycled Polypropylene (rPP)

PP is 100% recyclable and paintable. Reference Figure 1. Automotive batteries are recycled into building/home interior, exterior products. Some of these products are warranted by the manufacturer for over 25-years. Coating is the most preferred decorating process for mass customisation.

Industrial Liquid Coating of Polyolefin Products – Interior and Exterior Applications

Coating Technologies

Several coating technology options exist for OEM plastic finishing, each with distinct advantages depending on performance, cost, and line footprint requirements. These technologies fall into three main categories:

Single Component Lacquers: Easy to use with low per square foot cost, single component lacquers are commonly used in plastic decorating. These coatings dry and harden entirely by solvent or water evaporation and typically dry in 30 minutes or less at room temperature or under low bake conditions. Single component lacquers can be formulated for hardness and abrasion resistance, or alternatively for soft plastics can be made flexible and ductile. The ability to air dry at room temperature reduces capital investment requirements, although low baking at 100-120F helps reduce cycle time. Single component lacquers are best suited for finished products intended for use where potential exposure to condensing humidity, water immersion, and harsh chemicals is limited. These products are available in solvent and water-based formulations and can be applied with HVLP or air atomised spray.

Two component thermoset coatings: Two component thermosets offer high performance and can be optimised for a wide variety of extreme industrial duty, outdoor consumer goods, and automotive applications. Epoxies, polyurethanes, and to a lesser extent M-cure reactive modifiers dominate this realm. Polyurethane coatings are high in per square foot cost but offer excellent chemical resistance and automotive grade colour and gloss retention performance during prolonged direct sunlight exposure. Epoxies are lower in cost than urethanes, and excel in film hardness, chemical resistance, and moisture vapour barrier properties. However, epoxies have poor colour stability and durability when exposed to direct sunlight in topcoat applications and are susceptible to blushing, so are typically used as primers. Additionally, epoxy coated products are generally require a California Proposition 65 label.

Generally, two component thermoset coatings require long cure to handle/package time since most of the film hardness develops via chemical crosslinking (curing). Due to the heat sensitivity of plastic substrates, the ability to speed up curing involving two component thermosets by adding heat is limited. Plural component mixing equipment can enable the use of faster curing formulations when shorter cycle time is needed. For applications where cost or cure time constraints preclude the use of two component urethanes, M-cure is a potential option to consider since faster dry times can be achieved at ambient or low bake temperatures without the use of plural mixing equipment due to new M-cure resin technology that has enabled M-cure formulations to achieve much longer workable pot life than has historically been possible. Water-based and solvent based thermoset formulations are available and are typically applied with HVLP or air atomised spray.

UV Cured Coatings: UV cure coatings offer the best combination of fast drying/curing time and performance of any coating technology for plastic. Curing can typically be achieved in as little as 3-10 seconds depending on formulation and part geometry. Once cured, plastic products decorated with UV curable coatings are immediately ready for packaging. UV cure coatings excel in toughness and chemical resistance and can be formulated to achieve long term exterior durability or can be economised for lighter duty applications. UV cure coatings generally require direct line of sight exposure to a UV curing lamp to achieve film hardness, however water based UV cure coatings are unique in that they form a dry-to-touch film even before being cured, so small shadow areas on complex parts do not result in the presence of uncured, tacky residue in finished goods. Mercury vapour lamps are the most commonly used UV source for curing and can be microwave or arc generated. Arc style lamps are more cost effective to purchase but require warm up time and produce considerable heat. Microwave generated lamps are more expensive than arc lamps but are ready to use within seconds of being turned on, produce less heat, and have longer bulb life. Both microwave and arc lamps are available with iron or gallium doping, making them suitable for curing pigmented colours and can be combined with elliptical (flood) or parabolic (focused) reflectors depending on peak power requirements and part geometry. In addition to mercury lamps, LED UV lamps emerged as a competing technology offering instant on/off capability with very low energy usage and extremely low heat generation and are best suited to regularly shaped cylindrical parts or flat parts due to limitations in focal geometry. Additionally, while LED lamps excel in through-curing of highly pigmented or high build films, their use may require post-cure exposure to a diffuse or low power mercury lamp for complete surface cure. 100% solids, solvent based, and water-based formulations are available. UV coatings can be sprayed with HVLP or can be roll coated on flat surfaces.

Liquid Coating Selection Guide

Liquid Coating Selection Guide

Conclusion

Coating processes are multifaceted and require precise engineering and quality controls. The effects of paint chemistry and plastic compatibility, and surface quality are essential for product performance. Single component lacquer, two component thermosets and UV coating technologies are effective for painting & coating polypropylene materials, and they are available in waterbase chemistries.

References

  • Definitive Guide to Polypropylene, Omnexus SpecialChem, 2021
  • Sabreen, S. and Roobol, N: Painting Plastics for Painting, Plastics Decorating Magazine 2003
  • Sabreen, S. Inkjet Printing & Adhesion of Low Surface Energy Polymers, Plastics Decorating Magazine 2019

Scott R. Sabreen is founder and president of The Sabreen Group, Inc., an engineering consulting company specialising in secondary plastics manufacturing processes – surface pretreatments, adhesion bonding, inkjet printing, laser marking, industrial coatings, decorating and finishing, and product security. Sabreen has been developing pioneering technologies and solving manufacturing problems for more than 30 years. He can be contacted at 972.820.6777 or by visiting www.sabreen.com.

Dustin Kurath is the technical director of Northern Coatings and Chemical Co., a paint manufacturer specialising in high-performance industrial coatings. Kurath has been involved in coatings research on high-performance general industrial and automotive coatings, aerospace coatings, packaging coatings and radiation-curable coatings since the mid-2000s. Kurath can be reached at 906.352.5060 or at www.northern-coatings.com.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴