Technical Blog - The Sabreen Group, Inc.

Laser Marking Medical Tubing and Catheters: Depth Bands, Scales and Codes

Key Takeaways

  • Laser marking puts depth bands, scales and codes into the tube wall itself. There is no ink layer to flake, smear under a hydrophilic coating or add a new material to the patient-contact surface.
  • The compound decides the mark. Pebax, nylon, polyurethane, PVC, polyethylene, fluoropolymers and silicone all respond differently, and pigments, radiopaque fillers and laser additives change the result again.
  • UV (355 nm) lasers are the usual first choice because they change color with very little heat, which matters on walls a few thousandths of an inch thick.
  • A depth band has to go all the way around. That takes a rotary fixture, multiple marking heads or on-the-fly marking at the extrusion line, with band position held to a tolerance from the tip.
  • The mark is part of the device. It has to be qualified for contrast, wall integrity, sterilization, coatings and biological safety on the finished product.

Catheters, introducer sheaths, guiding catheters, endoscope shafts and feeding tubes all carry marks that a clinician reads during a procedure: bands that show how far the device has been inserted, graduated scales, numerals, orientation lines and identification codes. On a flexible tube with a thin wall, those marks are harder to produce than they look. This article covers how laser marking is used on medical tubing, how the tubing material and its additives control the result, which lasers suit the job, and what has to be proven before the process is released to production.

What Gets Marked on Tubing and Catheters

  • Depth bands. Rings around the shaft at fixed distances from the distal tip, often in single, double and triple groups so the clinician can count insertion depth at a glance.
  • Graduated scales and numerals. Centimeter marks with numbers along drainage, feeding, endotracheal and urology tubes.
  • Orientation and reference marks. Longitudinal lines or dots that show which way a curve, side port or lumen is facing.
  • Size and product identification. French size, length, brand and part number on the shaft, hub or strain relief.
  • Lot codes and UDI carriers. Human-readable lot numbers and Data Matrix codes, usually on a hub, connector or luer where there is a flat or rigid area. See Unique Device Identification (UDI).

Why Laser Instead of Ink

Pad printing and inkjet have marked tubing for decades, and they still do. Their weak points are well known. Most tubing resins have low surface energy, so the ink needs a plasma or corona pretreatment step, a cure step, and an adhesion test to prove it stayed on. The ink is one more material in contact with the patient. Ink also raises the surface slightly, which can interfere with a hydrophilic or lubricious coating applied over it.

A laser mark is a color change in the tube material. Nothing is added, nothing has to cure, and the layout is changed in software instead of by making a new printing plate. Our Knowledge Center documents medical tubing for invasive surgical procedures where on-the-fly laser marking replaced ink printing, using FDA-approved laser additives. The trade-off is that the laser process depends heavily on the compound, so the material has to be part of the design from the start. A broader comparison is in laser marking vs. inkjet printing.

How Tubing Materials Respond

The table is a starting guide. Color, radiopaque filler and additive package can move any material up or down.

Tubing material Typical response Notes
Polyether block amide (Pebax) and nylon 11/12 Good dark marks with UV; contrast with fiber lasers usually needs an additive The most common catheter shaft materials. See laser marking nylon
Thermoplastic polyurethane (TPU) Good with UV; aromatic grades mark more readily than aliphatic See polyurethane
Flexible PVC Marks dark with UV and fiber lasers Plasticizer and stabilizer packages vary; fume extraction is mandatory. See laser marking PVC
Polyethylene and polypropylene Weak on natural grades Normally needs a laser additive for a readable mark
PTFE, FEP and other fluoropolymers Difficult; pigmented or additive-filled grades mark with UV See laser marking PTFE
Silicone Difficult on clear grades; pigmented grades can mark with UV Laser-markable silicone compounds exist; trial the exact grade
PEEK and polyimide Naturally absorbing; mark dark Thin walls need low energy to avoid charring through

Pigments and fillers matter as much as the base resin. Titanium dioxide, the standard white pigment, absorbs strongly in the ultraviolet, so white and pastel tubing often gives a clean gray-to-black mark at 355 nm. Radiopaque fillers such as barium sulfate, bismuth compounds and tungsten are loaded at high percentages and change how the wall absorbs and conducts heat; some bismuth compounds improve the mark, while a heavily filled wall can turn rough if it is overheated. Clear and translucent tubing has little to absorb the beam and is the hardest case, as described in laser marking clear and transparent plastics. The general mechanism is covered in how colorants and pigments change laser marking results.

Where the standard compound will not mark, a laser marking additive compounded into the tubing resin gives the beam something to couple with. For a medical device the additive must have the regulatory status the application needs, and it has to be included in the material and biological evaluation of the device.

Choosing the Laser

  • UV, 355 nm. The workhorse for tubing. Most polymers and pigments absorb ultraviolet directly, so the color change happens in a very shallow layer with little heat. This is what is meant by cold laser marking. The surface stays smooth, which matters for anything that slides through a vessel or a sheath.
  • Fiber and vanadate, 1064 nm. Faster and lower in cost per watt, and well suited to hubs, connectors and thicker tubing made from an additive-containing compound. On thin, unmodified walls the heat input is harder to control.
  • Green, 532 nm. A middle option for some materials that respond poorly at 1064 nm.
  • CO2, 10.6 µm. Melts or engraves the surface without much color change. Removing wall material from a catheter is rarely acceptable.

The two main choices are compared in UV vs. fiber laser marking.

Marking All the Way Around

A depth band that only covers part of the circumference can be turned away from the clinician. Three approaches give full coverage:

  • Rotary indexing. Cut lengths or finished catheters are held in a collet or on a mandrel and rotated under one marking head. Flexible, accurate, and the slowest of the three.
  • Multiple heads. Two or three heads spaced around the tube mark overlapping arcs at once with no rotation. This suits high volumes and long shafts that are awkward to spin.
  • On-the-fly at the extrusion line. The laser marks the tube as it moves, using an encoder to track line speed. This is the lowest-cost route for scales and repeating bands on continuous tubing.

Position is the tolerance that causes the most trouble. Bands are dimensioned from the distal tip, and a soft tube stretches under its own handling tension. Fixtures that support the tube without pulling it, a vision or mechanical datum on the tip, and marking after tipping and cutting instead of before all help hold the numbers. A mandrel inside the lumen keeps the tube round and also acts as a heat sink.

Protecting a Thin Wall

Catheter walls are often 0.1 to 0.25 mm thick, and some are thinner. A mark that looks perfect can still have damaged the tube, so set the process limits by what the wall tolerates, then find the best contrast inside those limits.

  • Surface roughness. Foamed or raised marks add friction and can disturb a hydrophilic coating. Aim for a smooth color change and measure it.
  • Mechanical strength. Check tensile, burst and kink performance on marked samples against unmarked controls, especially where a band sits on a thin distal section.
  • Particulate. Overheated marks can shed debris. Low pulse energy, good extraction and a particulate test address this.
  • Underlying layers. Many shafts have a braid, coil or liner under the outer jacket. The beam must not reach it or bond the jacket to it unevenly.

The parameter relationships are the same as on molded parts and are explained in process parameters affecting mark quality.

Qualifying the Marking Process

For a regulated device, the question is not only whether the mark is readable today. Plan to show the following on finished, packaged and sterilized product:

  • Legibility and contrast after sterilization by the method actually used. Ethylene oxide, gamma and e-beam affect polymers and color differently, and some marks shift or fade. Include aged samples; see accelerated aging.
  • Coating compatibility. If a hydrophilic or lubricious coating goes over the mark, confirm coating adhesion and mark legibility together.
  • Biological safety. Laser marking changes the surface chemistry in the marked area, so the marked device, not just the raw tubing, belongs in the biological evaluation under ISO 10993.
  • Dimensional accuracy of band and scale positions, with a measurement method that has been checked for repeatability.
  • A validated process. Installation, operational and performance qualification with defined parameter limits. See IQ, OQ and PQ for a laser marking process and ISO 13485 and a qualified marking process.

Any later change of resin lot source, colorant, radiopaque filler or extrusion supplier should trigger a review, because each can move the mark. Guidance on that decision is in when a process change needs revalidation.

Related Reading

Need help with this?

The Sabreen Group helps medical device manufacturers and tubing extruders develop laser marking processes for catheters and tubing, from compound and laser additive selection to parameter development and qualification. See our plastics laser marking services and medical and pharmaceutical work, or contact us to discuss your application.

Frequently Asked Questions

Can you laser mark catheter tubing?

Yes. Most catheter materials, including Pebax, nylon, polyurethane and PVC, can be laser marked, most often with a UV laser. The result depends on the exact compound, its color and its fillers, so trials should be run on production tubing.

Which laser is best for marking medical tubing?

A UV laser at 355 nm is the usual first choice because it produces a color change with very little heat and leaves the surface smooth. Fiber lasers at 1064 nm are used on hubs, connectors and tubing made from compounds that contain a laser additive.

How are depth bands marked all the way around a catheter?

Either the catheter is rotated under one marking head, or two or three heads placed around the tube mark it at the same time. Continuous tubing can also be marked on the fly at the extrusion line.

Does laser marking weaken thin-wall tubing?

A properly developed mark changes only a very shallow surface layer and does not measurably affect strength. Too much energy can roughen or thin the wall, so tensile, burst and surface tests on marked samples are part of process development.

Do laser marks on tubing survive sterilization?

They normally do, but it has to be confirmed for the specific material and sterilization method. Ethylene oxide, gamma and e-beam affect polymers differently, and contrast should be checked after sterilization and aging.

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.