Adhesion Bonding, Contact Angle, and Surface Properties of Polyamide Nylon

Polyamides, also known as nylons, are high-performance plastics with excellent chemical resistance. Nylons are hygroscopic and absorb moisture from the air. Moisture in and of itself causes adhesion problems. Nylon is hydrophobic and has low surface wettability. Question – Is nylon hydrophobic, hydrophilic, or maybe both?

A polyamide is a polymer containing repeating amide (–CO-NH–) linkages. The manufacturing of different polyamide types varies depending on their monomeric units. They may be aliphatic, semi-aromatic, and aromatic (aramids). Based on their crystallinity they may be amorphous, semi-crystalline, or crystalline. Nylon polymers are inherently difficult to bond because they are hydrophobic, chemically inert, and possess poor surface wettability (i.e., low surface energy). Furthermore, nylons are hygroscopic and will absorb moisture in excess of 3% of their mass of water from the atmosphere. Moisture, in and of itself, causes

adhesion problems.

Wait, the statements above appear to be directly contradictory. Is nylon hydrophobic or hydrophilic? The apparent paradox is resolved by recognising that nylon’s hydrophobic behaviour is a surface property and its hydrophilic behaviour is a bulk property. Polyimide also exhibits this behaviour.

Examining the chemical structure of a polymer’s repeat unit, such as Methyl (CH3) hydrophobic polyolefins or Amide hydrophilic nylons, is a simple way to determine whether it is hydrophilic or hydrophobic. The simplest method to determine the surface properties of a polymer is to conduct water contact angle measurements for static contact angle and dynamic contact angle.

Key Takeaways

  • Nylon is hydrophobic at the surface and hydrophilic in bulk — the apparent contradiction is the key to understanding it.
  • Nylons absorb over 3% of their mass in water from the atmosphere, and moisture alone causes adhesion problems.
  • Amide linkages attract water, which drives the bulk behaviour; the surface remains low energy and non-wetting.
  • Polyimide behaves the same way, so the principle generalises beyond polyamide.
Adhesion Bonding, Contact Angle and Surface Properties of Polyamide Nylon

Nylon, like most polymers, has a low surface energy. This is due to the surface chemistry and surface and physics of polymers. Contact angles are considered to be affected by both changes in surface chemistry and changes in surface topography. When a droplet is attached to a solid surface and the solid surface is tilted, the droplet will lunge forward and slide downward. The angles formed are respectively termed the Advancing Angle and the Receding Angle. ASTM D724 describes methods for measuring DCAs using advanced equipment (optical tensiometers and goniometers) to analyse advancing and receding contact angles based on drop shape analysis and mass.

The advancing contact angle is most sensitive to the low-energy (unmodified) components of the substrate surface, while the receding angle is more sensitive to the high energy, oxidised groups introduced by surface pretreatments. Thus, the receding angle is actually the measurement most characteristic of the modified component of the surface following pretreatments. Therefore, it is critical to measure both the advancing and receding contact angles on all surface-modified materials.

Scott R. Sabreen is founder and president of The Sabreen Group, Inc., which is an engineering company specialising in secondary plastics manufacturing processes – surface pretreatments, bonding decorating and finishing, laser marking and product security. He has been developing new technologies and solving manufacturing problems for over 30 years. Sabreen can be contacted at 972.820.6777 or by visiting www.sabreen.com or www.adhesionbonding.com.

Frequently Asked Questions

Is nylon hydrophobic or hydrophilic?

Both, and that is not a contradiction. Nylon’s hydrophobic behaviour is a surface property while its hydrophilic behaviour is a bulk property. The surface resists wetting and has low surface energy; the amide groups within the chain attract water, so the bulk absorbs moisture readily.

How much moisture does nylon absorb?

In excess of 3% of its mass from the atmosphere. Moisture in and of itself causes adhesion problems, which is why proper drying before moulding is critical to both processing and the performance of any subsequent bonding step.

How can you tell whether a polymer is hydrophilic or hydrophobic?

Examine the repeat unit of its chemical structure. Methyl groups, as in polyolefins, indicate hydrophobic behaviour; amide groups, as in nylons, indicate hydrophilic behaviour. It is a quick first-order check before any surface testing.

Why are nylons difficult to bond?

They are hydrophobic, chemically inert and have poor surface wettability from low surface energy. Adhesives cannot wet out the surface adequately, so pretreatment is normally required to raise surface energy and add polar chemical functionality.

Does polyimide behave the same way as nylon?

Yes. Polyimide exhibits the same split between hydrophobic surface behaviour and hydrophilic bulk behaviour, so the same drying discipline and pretreatment logic applies.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴