Laser Marking of Polypropylene and Polyethylene Plastics Using Fibre Lasers

Laser marking and engraving on polyolefin plastics, such as polypropylene and polyethylene, is difficult due to their polymeric properties, and there are different types ranging from homopolymer and copolymer polypropylenes including HDPE, LDPE, LLDPE and others that intrinsically mark differently. When developing a product to be laser marked, engineers should consider which grade is best in terms of performance and markability. MOPA Ytterbium fibre lasers are ideal for marking polyolefin plastics because of their capability to produce short pulse widths to create scratch resistant dark and light-coloured marking contrast. Long pulse widths more than 100ns can cause excessive burning.

Recent advancements in colourant technology, such as laser-specific carbon blacks and titanium dioxides, as well as foaming agents, provide superior contrast quality, line edge detail, and the fastest speed, including “on-the-fly” marking. These attributes make them ideal for laser marking wire and cable insulation in automotive, construction, medical, packaging, piping, and other applications.

Key Takeaways

  • Polyolefins need additives. PP and PE absorb near-infrared poorly, so unmodified material gives weak contrast at any power.
  • Grades mark differently. HDPE is generally easiest; polyethylene is generally easier than polypropylene.
  • MOPA fibre lasers with short pulse widths are preferred; pulses beyond about 100 ns cause excessive burning.
  • Two surface reactions apply — carbonisation (charring) and chemical change (foaming).
  • Inline marking is fast. Wine corks and linerless closure undercaps run at up to 2,000 pieces per minute.
sabreen polypropylene laser marking collage

Optimal laser marking. Laser marking on polypropylene and polyethylene plastics normally require laser-sensitive additives incorporated into optimised colourant compounds, colour concentrates or precompounded. Flame retardants are commonly used in wire/cable and insulator products which affect colourmatch and compound formulations. Additives such as antimony-doped tin oxide and antimony trioxide impart a “grayish” tint to the natural (uncoloured) substrate opacity. Other additives can contain aluminium particles, mixed metal oxides and proprietary compounds. Colour adjustments are made using pigments and dyes to achieve the final colourmatch appearance.

When properly blended, laser marking additives, compounds, and colourants have no adverse impact on polymer properties, meet requirements such as UL, NEMA, FDA, RoHS and Yellow Card, and do not require recertification. The chemical components of laser optimised formulations are influenced by a number of factors, including polymer type and colour, marking contrast colour, surface reaction mechanism type, and laser wavelength. Two types of surface reactions when laser marking polyolefins are Carbonisation “charring” and Chemical change “foaming”.

Inline “on-the-fly” laser marking on polyolefin products provide state-of-the-art manufacturing advantages. Marking speeds for wine corks and undercap promotions on linerless beverage closures are capable of 2,000 pieces per minute for alphanumeric text and graphics. Equally impressive results are achieved on extruded medical and wire/cable products.

Laser Markability of Polyolefins

Polyolefins have different surface reaction mechanism temperatures than other polymers, necessitating the use of specialised formulations. Even polyolefins from the same family, such as polyethylene and polypropylene, laser mark differently. This is one reason why High-density polyethylene is generally the easiest to mark. Polyethylene plastics are generally easier to mark than polypropylenes.

Polyolefin is a class of polymers formed from olefins. This versatile group of materials includes well-known polymers like polyethylene (PE) and polypropylene (PP), which are widely used in a variety of industries due to their outstanding chemical and physical properties. The four most popular varieties of polyolefins are low-density polyethylene, linear low-density polyethylene, high-density polyethylene, and polypropylene.

Not All Plastics and Lasers Produce Identical Marks!

The quality of laser components, optics, scan-heads, and versatile software is critical. Industrial lasers are superior to cheap wholesale (resellers) hobbyist-type lasers. Cheap lasers have serious problems with erratic marking quality, as well as low-cost optics and electronics, resulting in variations in beam quality and inconsistent marking.

Some laser equipment resellers and manufacturers’ websites use internet buzz terms about polyolefins to gain “clicks” and high rankings – they are not experts in polymers, colourants and the chemical interaction pathways with various laser wavelengths which are critical for achieving optimised laser marking quality. Robust and cost-effective laser solutions integrate polymer material science with the optimal laser source (wavelength).

Contact The SABREEN Group. Bring us your toughest laser marking challenges!

Frequently Asked Questions

Why is polypropylene harder to laser mark than polyethylene?

Polyolefins have different surface-reaction temperatures from other polymers, and even within the family the thresholds differ. Polyethylene generally reacts more readily, with HDPE the easiest of all, while polypropylene needs more carefully matched formulations.

Can polypropylene be marked without additives?

Not to production contrast standards. Effective marking on PP and PE normally requires laser-sensitive additives incorporated into optimised colourant compounds, colour concentrates or precompounded resin.

Do flame retardants interfere with laser marking polyolefins?

They complicate it. Flame retardants are common in wire, cable and insulator products and they affect colour match and compound formulation, so the laser additive package has to be developed alongside them rather than added afterwards.

What pulse width should be used on polyolefins?

Short. MOPA ytterbium fibre lasers are preferred because they produce the short pulse widths needed for scratch-resistant dark and light contrast. Pulse widths longer than about 100 nanoseconds tend to cause excessive burning.

How fast can inline polyolefin marking run?

Very fast. Marking speeds for wine corks and undercap promotions on linerless beverage closures reach 2,000 pieces per minute for alphanumeric text and graphics, with comparable results on extruded medical and wire and cable products.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴