Innovations in Plastics Products Security: Anticounterfeiting Technologies

Counterfeiting is a worldwide epidemic. It threatens the global economy and public health through the production of inferior products that circumvent consumer protection regulatory channels. Spending by the public and corporations is increased to counter the illegal trade, and prices of legitimate products increase as companies seek to recover their financial losses. The International Chamber of Commerce estimated that in 2015, the value of counterfeit goods globally exceeded $1.7 trillion. That represents more than two percent of the world’s current total economic output. With profits, corporate liability and brand reputations at stake, companies are fighting back to protect their brands. Decades of experience and information derived from reputable global sources clearly demonstrate that no single anticounterfeit technology works best for all products and situations. Multiple approaches and solutions are needed, i.e., a layered approach works best. This article examines “overt” and “covert” security authentication solutions.

Key Takeaways

  • Counterfeit goods exceeded $1.7 trillion in 2015, over 2% of world economic output.
  • Overt features are user-verifiable, but only against a genuine reference sample of the feature.
  • Features must self-destruct on removal. Overt and covert solutions are designed so they cannot be reused or removed without defacing the pack.
  • OVDs resist copying entirely — they cannot be photocopied, scanned or accurately reproduced.
  • Partial de-metallisation adds a second layer, chemically removing reflective material to outline the image, as used on banknotes.

Frequently Asked Questions

What is the practical difference between overt and covert features?

Overt technologies can be verified by users, typically visually, provided they are familiar with the feature and have a genuine reference sample to compare against. Covert technologies require detection equipment. Both are designed so they cannot be reused or removed without defacing or damaging the pack.

Why is a reference sample so important for overt features?

Because verification is comparative. Without a genuine example to compare against, an untrained observer cannot reliably distinguish a good imitation from the real feature — which is why an overt device is often incorporated within a tamper-evident feature for added security.

How do optically variable devices work?

They present complex images that exhibit different optical effects depending on how much light strikes them and the viewing angle, sometimes with an illuminating light source as an additional benefit. Effects include image flips or transitions, colour transformations and monochromatic contrasts.

What is partial de-metallisation?

A process where some of the reflective backing layer is chemically removed to give an intricate outline to the image, as seen on banknotes. The layer can be made so thin as to be transparent, producing a clear film with a ghost reflective image visible at certain angles.

What does a complete protection strategy require?

Implementing overt, covert and forensic technologies together, so criminals cannot reuse, copy or misappropriate products. Depending on the product’s importance and value, combining overt and covert features provides layered protection.

Anticounterfeiting Technology Classifications

Anticounterfeiting technologies can be classified and explained in different ways. In this article, technology classifications are shown on the basis of usage.

Authentication

Authentication is the act of establishing or confirming something as genuine. ISO 12931:2012 specifies performance criteria and evaluation methodology for authentication solutions used to establish material good authenticity throughout the entire product life cycle. However, it does not specify how technical solutions achieve these performance criteria. Authentication generally is done through the overt or covert features in the product. Depending upon the importance and value of the product, combining overt and covert features provides layered protection solutions.

Anti-counterfeit Technologies – Overt and Covert

Overt and covert security authentication is examined in this article. The main difference between the two is that overt technologies can be verified by users (typically visually) who are familiar with the overt technology and have a reference genuine sample of the feature with which to compare the suspect feature on the suspect product. Overt and covert solutions are designed to be applied in such a way that they cannot be reused or removed without being defaced or causing damage to the pack. For this reason, an overt device might be incorporated within a tamper-evident feature for added security.

Overt techniques are clearly visible and do not require detection devices because they are based upon the sensorial capability of the human being. Note: overt technologies also can be used as covert technologies and vice versa, depending on the complexity of the design. Most of the recent developments in overt and covert technologies have embedded hidden features to make them more difficult to be illegally replicated.

Overt technologies include the following:

  • 2D/3D holography (morphing, flip image, gradient, pseudo colour, grayscale image, linear/circular kinetic)
  • Optical variable devices
  • Watermark
  • Security graphics (micro/nano text, security patterns, multicolour designs, deliberately integrated errors)
  • Security threads
  • Security foils
  • Colour shifting inks
  • Intaglio printing
  • Laser marking
  • Fluorescence artifacts
  • Coloured interlayers
  • 2D codes (QR, data matrix)
  • Sequential product numbering, serialisation
  • Contact microchip
  • Photograph
  • Magnetic strip

Covert technologies typically require specific equipment to be verified, as the details of the technology are not disclosed. Some covert technologies – such as infrared (IR) and ultraviolet (UV) inks, microtext and microscopic tagging – are invisible and difficult to detect and replicate without special detection equipment. Images printed with UV inks are only visible under a UV lamp. UV inks are available in different frequencies, thus ? depending on the formulation of the ink – the investigators will need to use either a long-wave or short-wave UV lamp for the printed images or text to become visible. UV inks may fluoresce in a variety of colours, adding to the complexity of this covert feature.

Covert technologies include the following:

  • Micro/nano printing
  • Hidden imagery
  • Polarisation imagery
  • Taggants and chemicals, up-converting phosphors
  • Security inks
  • Nanoparticles

In addition, covert technologies, such as taggants, also can be placed onto packaging, with the most effective being completely invisible and only detectable with a special reading device. As with other covert technologies, taggants only can be identified by the brand owner or people they equip with the appropriate knowledge and technology to provide conclusive verification.

Featured Technology: Innovations in Optically Variable Devices

Optical Variable Devices (OVDs) are a relatively new form of security technology. Complex images exhibit various optical effects depending on the amount of light striking the OVD and the angle in which the OVD is viewed. Sometimes an illuminating light source is used as an additional security benefit. OVDs cannot be photocopied or scanned and cannot be accurately replicated or reproduced. Figure 2 demonstrates optically variable inks with colour shifting effects when viewed under reflected and transmitted light conditions.

Another example of OVD security, as shown in Figure 3, demonstrates optically variable inks with polarising effects.

Properties of Optical Variable Devices

OVDs, similar to holograms, generally involve image flips or transitions, colour transformations and monochromatic contrasts. OVDs typically are composed of a transparent film (as the image carrier) and a reflective backing layer, which usually is a very thin layer of aluminium or copper that produces a feature characteristic hue. Additional security features may be added by the process of partial de-metallisation, whereby some of the reflective layer is chemically removed to give an intricate outline to the image, as seen on banknotes. The reflective layer can be so thin as to be transparent, resulting in a clear film with more of a ghost reflective image visible under certain angles of viewing and illumination.

Ultra high-resolution micro/nano images (10-micron and smaller, 62,000 characters per cm2) are one of the important breakthroughs in optical security, using beam-steered lasers. This detail exceeds the resolution available via any other copying, printing or scanning device in industry. Features can be visible to the naked eye, while fine detail only can be viewed using hand-held magnification. The risk of counterfeiting has been greatly reduced by recent advances in the production of micro/nano images and security patterns, which now can be resolved at more than double the previous level.

  • OVDs can be placed on the surface of products (typically by stamping or rolled laminator process) or under the surface of products (by laminating or injection moulding).
  • OVDs can be metallised (shiny) or transparent (HRI – High Refractive Index).
  • Some OVDs are a combination of metallised and transparent (like the US Passport Card).
  • When laser marking is done on HRI type OVD, the laser passes through the transparent OVD.
  • When laser marking is done on a metallised OVD, the laser ablates the metallisation, creating a unique or personalised OVD.
  • OVDs can be manufactured to fracture when attempts are made to remove them from the product. This is a tamper-evident feature that helps keep counterfeiters from removing or reusing OVDs.

Conclusion

In today’s global economy when products are under attack in forms of counterfeiting and tampering, authentication technologies play a vital role in protecting brand reputation and the public. With the use of increasingly sophisticated counterfeit methods, criminals continue to advance and profit at the cost of public safety and company revenue. It is essential to implement overt, covert and forensic technologies to ensure that criminals are unable to reuse, copy or misappropriate products.

Scott R. Sabreen is founder and president of The Sabreen Group, Inc., an engineering company specialising in secondary plastics manufacturing processes ? laser marking, surface pretreatments, bonding, decorating and finishing, and product security. Sabreen has been developing pioneering technologies and solving manufacturing problems for over 30 years. He can be contacted at 972.820.6777 or by visiting www.sabreen.com or www.plasticslasermarking.com.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴