Through-Transmission Laser Welding

August 29, 2026
8 min read

Key Takeaways

  • One part transmits, the other absorbs. The beam passes through the upper component and deposits its energy at the interface.
  • Heat is generated only where it is wanted, so the process adds no vibration and no particulate.
  • Fit-up decides weld quality once absorption is adequate — a gap cannot be closed with more power.
  • Carbon black is the traditional absorber, which is why so many laser-welded assemblies are dark.

Through-Transmission Laser Welding

Through-transmission laser welding is a joining process in which a near-infrared beam passes through a transmissive upper component and is absorbed at the surface of a lower component, generating heat precisely at the joint interface so that both faces melt and fuse under clamping pressure. It is the dominant laser welding configuration for thermoplastics, and the reason the technique is viable at all on materials that would otherwise be damaged by surface heating.

The value of the arrangement is that energy is deposited inside the assembly
rather than on its outside. Nothing on the visible surface is heated appreciably, so cosmetic
faces survive intact, and no mechanical energy is applied to the assembly at all —
which is why the method suits enclosures containing electronics, sensors or fluid paths that
ultrasonic or vibration welding would disturb.

What Each Half of the Joint Must Do

Transmissive part Absorbing part
Optical requirement Pass the beam to the interface with minimal loss Absorb the beam at or very near its surface
What defeats it Wall thickness, pigment loading, glass filler, crystallinity, moulded-in weld lines Insufficient absorber loading, or absorber that is dispersed too deeply
Usual approach Natural or lightly pigmented resin; amorphous polymers transmit better than semi-crystalline Carbon black, or a dual-purpose additive where colour matters
Most common oversight Assuming a clear-looking part transmits well — visible clarity and near-infrared transmission are different properties Assuming loading tuned for marking contrast will also serve the weld

Both parts should normally be the same polymer, or polymers of demonstrated compatibility.
Dissimilar materials with different melt temperatures and viscosities rarely produce a sound
weld regardless of the optical arrangement.

Joint Design and Fit-Up

Once absorption is adequate, weld quality is a mechanical question. This is where most
programmes actually succeed or fail:

  • Intimate contact is mandatory. The melt has to bridge the interface, and
    a gap gives it nothing to bridge to. Adding energy across a gap burns material rather than
    welding it.
  • Gap tolerance is tighter than for ultrasonic or vibration welding. Part
    warpage and moulding tolerance have to be controlled to the joint specifically, not merely
    to the overall part dimensions.
  • Design a locating joint. A step, tongue-and-groove or shear joint
    positions the parts and concentrates melt where it is wanted, instead of relying on flat
    faces meeting perfectly.
  • Clamping must be uniform along the weld path. Uneven pressure produces a
    weld that is strong in some places and absent in others.
  • The clamping tool sits in the beam path. Glass or acrylic pressure plates
    must be kept clean and unscratched, because their condition directly changes delivered
    energy.
  • Keep the weld path away from gates and moulded weld lines in the
    transmissive part, which scatter the beam locally and produce a repeatable weak spot.

Welding Strategies

Strategy How it works Best suited to
Contour welding The beam traces the joint path once, melting progressively Large or complex two-dimensional paths; flexible, lower tooling cost
Quasi-simultaneous The beam scans the whole path repeatedly at high speed, so the entire joint melts together Assemblies needing joint collapse and a hermetic seal; tolerates minor gaps better
Simultaneous Fixed diode arrays or a masked source heat the entire joint at once High volume, fixed geometry; shortest cycle time, highest tooling cost
Radial and mask welding Rotational or masked exposure Cylindrical parts, or very fine feature definition

Diagnosing Weld Defects

Symptom Likely cause Correction
Weak weld with correct absorber loading Fit-up, not optics Check clamping pressure and joint gap before raising power.
Strength varies along the joint line Transmission varying through the upper part Measure transmission across the transmissive component; wall thickness and pigment dispersion both show here.
Voids or burning at the interface Excess energy, or dwell too long at a point Reduce power or raise traverse speed. Voids are trapped decomposition gas.
A repeatable weak spot at one location Gate mark or moulded weld line scattering the beam Relocate the gate, or route the weld path away from the feature.
Welds degrade over a production run Clamping glass fouling or scratching Clean and inspect the clamp on a schedule — it is an optical component.
Passes assembly test, leaks in service Qualified on initial strength only Add thermal cycling and chemical exposure to the qualification, and examine failure mode rather than load alone.
Cannot weld a light-coloured assembly Carbon black is the only absorber considered Specify a dual-purpose or near-infrared-absorbing additive that is not visually black.

Related Terms and Reading

Applying this in production

The Sabreen Group provides independent engineering support for through-transmission weld development, material pairing and joint qualification. If you are specifying a process, qualifying a material or troubleshooting a production problem, our engineering services team can help. Contact us to discuss your application.

Frequently Asked Questions

Why must one part transmit and the other absorb?

So that heat is generated at the joint interface rather than on the outside of the assembly. The beam passes through the upper component without depositing appreciable energy, is absorbed at the surface of the lower one, and the resulting heat melts both faces together under clamping pressure. That is what allows cosmetic surfaces and internal components to survive a process that is welding a few millimetres away.

Does a clear part necessarily transmit the beam well?

No, and the assumption causes a lot of wasted development. Visible clarity and near-infrared transmission are different properties: a part can look water-clear and still attenuate at 1064 nm, and a semi-crystalline polymer scatters the beam through its crystalline regions regardless of how it looks. Measure transmission at the working wavelength rather than judging by eye.

Why is the weld weak when absorber loading is correct?

Usually fit-up. The faces must be in intimate contact under clamping pressure because the melt has to bridge the interface; where there is a gap, extra energy burns the material rather than closing it. Laser welding tolerates gaps less well than ultrasonic or vibration welding, so joint tolerance and part warpage have to be controlled specifically at the weld.

Must a laser-welded assembly be black?

Not any longer. Carbon black is the traditional absorber and remains the cheapest, which is why so many laser-welded assemblies are dark, but dual-purpose and near-infrared-absorbing additives now provide absorption without being visually black. That allows light, coloured and in some systems near-clear welded assemblies, at a higher additive cost.

Which welding strategy should be chosen?

Contour welding suits large or complex paths with modest tooling cost; quasi-simultaneous scanning melts the whole joint together, which allows joint collapse and tolerates minor gaps better, making it the usual choice for hermetic seals; simultaneous welding gives the shortest cycle for high-volume fixed geometry at the highest tooling cost. Gap tolerance and volume normally decide it.

Avatar

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

To arrange a teleconference with Scott Sabreen, please fill out the information below.

What is your mailing address?

Topic of interest?

What industry are you in?

What is the primary plastic type?

Submission Successful!

Your message has been received. We will be in touch shortly to arrange a meeting time.

We Have Received Your Request

We have received your request and will be in touch shortly.