Surface Pretreatments / Surface Quality - The Sabreen Group, Inc.

Pyrosil Flame Plasma Treatment for Indian Manufacturers

PYROSIL treatment is a combustion chemical vapour deposition (CCVD) process utilised to improve adhesion on surfaces to be bonded, a solution increasingly sought by manufacturers across India for demanding bonding applications. PYROSIL is a glow-discharge plasma process conducted at ambient conditions. PYROSIL treatment is a surface modification technique that deposits an amorphous silicon dioxide (SiO2) layer on a substrate surface via Combustion Chemical Vapour Deposition (CCVD). SURA Instruments GmbH developed the equipment and processes in the 1980’s that lead to the first successful commercialisation of the technology used to increase bonding with adhesives. By means of flame-pyrolysis, a thin layer (5 – 100 nm) of highly reactive and hydrophobic silicone oxide can be achieved on the substrate. Consequently, a defined hydrophilic surface is built due to the high density of Si-OH groups on the surface of the deposited SiO2 particles and nanoscale roughness. Silicon-containing films find many applications for polymers, glass, ceramics & metals. In the process, the product to be treated is fed through a laminar gas flame, doped with a silicon-containing precursor material (PYROSIL), in a manner similar to traditional flame treatment. Due to the brief flame-substrate interaction the process can be used on temperature sensitive plastics materials.

Pyrosil® process is a combustion deposition.
Pyrosil Flame Plasma - The Sabreen Group, Inc.
Propane flame (left) and Pyrosil flame process (right)

Combustion Chemical Vapour Deposition (CCVD) is a chemical process by which thin-film coatings are deposited onto substrates in the open atmosphere. In the CCVD process, a precursor compound is added to the burning gas. The flame is moved closely above the surface to be coated. The high energy within the flame converts the precursors into highly reactive intermediates, which readily react with the substrate, forming a firmly adhering deposit. The microstructure and thickness of the deposited layer are controlled by process parameters including speed of substrate or flame, number of passes, substrate temperature and distance between flame and substrate. Silicon dioxide layers are the most commonly deposited layers. Freshly deposited layers are highly reactive and can thus serve as adhesion promoting layers for polymer coatings and bonding.

PYROSIL Versus Flame Treatment

PYROSIL and traditional flame plasma treatment have process similarities, but the flame chemistry and surface functionality mechanism are different. Both methods are gas-phase surface oxidation processes in which the combustion of a hydrocarbon fuel, under controlled conditions, generates the flame plasma that modifies the substrate surface. Premixed laminar flames produce an exothermic reaction. The PYROSIL flame is pinkish on colour while the traditional flame treatment colour is bluish in colour. Reference Photo 1. The main difference is that PYROSIL produces SiO2 and flame treatment does not. Consequently, a defined hydrophilic surface is built due to the high density of Si–OH groups on the surface of the deposited SiO2 particles. Similar combustion equipment, ribbon burners and process setup/control are utilised. The three main process control variables are flame chemistry, distance of the substrate from the flame and dwell time of treatment. Treatment must take place in the main reaction luminous zone or oxidising.

For PYROSIL, one equation for the combustion of organosilicon compound tetramethysilane “TMS” and the formation of SiO2 is:

Si(CH3)4 + 13 O2 + C3H8 — SiO2 + 10 H2O + 7 CO2

For natural gas flame treatment, the following equation describes the combustion reaction:

CH4 + 2O2 + 8N2 — CO2 + 2H2O + 8N2

Both combustion reactions produce CO2 and H2O water byproducts.

Atmospheric Plasma

Flame Plasma

UV Radiation Ozone

Electrical Corona Discharge

Fluorooxidation

Electrical Air Plasma

Cold Gas Plasma

Chemical & Mechanical


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴