Electrical Air Plasma

Key Takeaways

  • Ambient air is the working gas, so no specialty gas supply or cylinders are needed.
  • It runs in open air with no vacuum chamber, suiting continuous production lines.
  • Three system types: corona discharge, atmospheric pressure plasma, and plasma jet configurations.
  • Activation decays over time. Surface energy gains degrade unless the part is bonded or coated promptly.

Electrical Air Plasma

Electrical air plasma is an atmospheric-pressure surface pretreatment that uses ambient compressed air as the process gas, ionising it electrically to oxidise and activate polymer surfaces immediately before bonding, printing or coating. It requires no vacuum, no bottled gas and no combustible fuel — clean dry compressed air and electrical power are the only inputs, which makes it one of the simplest pretreatments to integrate into an existing production cell.

Mechanism

An electrical discharge within the treatment head ionises the air stream, generating oxygen radicals, ozone, excited nitrogen species and UV. Directed at a polymer surface, these species break carbon–hydrogen bonds in the top few molecular layers and graft oxygen-containing polar groups in their place. Surface energy rises immediately, contact angle falls, and adhesives, inks and coatings wet the surface instead of beading on it.

The same discharge simultaneously ablates the weak boundary layer of mould release agents, slip additives and airborne oils that otherwise dominate adhesion failure. In practice this cleaning contribution is often as important as the chemical activation itself — a point examined in Sabreen’s discussion of adhesion failures.

Key Process Parameters

Parameter Practical guidance
Standoff distance Usually 5–20 mm. The single most sensitive variable; reactive species recombine quickly in open air.
Dwell / traverse speed Set to give consistent exposure. Under-treatment gives no bond; gross over-treatment degrades and weakens the surface layer.
Air quality Must be clean, dry and oil-free. Compressor carry-over deposits oil on the very surface being cleaned.
Part fixturing Repeatable presentation matters more than raw power — varying standoff produces varying dyne level across the part.

Strengths and Limits

  • Inline and robot-compatible. Heads are readily mounted on a robot arm or conveyor for treatment of moulded three-dimensional parts.
  • Selective treatment. Only the bond area need be activated, which preserves the untreated appearance and printability of the remainder of the part.
  • No open flame. Where a combustion process is unacceptable on safety or facility grounds, electrical air plasma is the practical substitute for flame plasma.
  • Line-of-sight limited. Recesses, undercuts and internal surfaces are shadowed; those geometries point toward low-pressure cold gas plasma.
  • Ozone generation. Local extraction is normally required.
  • Treatment decays. Surface energy falls over hours to days as polymer chains reorient, so bonding should follow treatment promptly.

Confirming the Result

Treatment level should be verified rather than assumed. Wetting tension solutions to ASTM D2578 give a rapid dyne reading at the workstation; contact angle goniometry provides the quantitative value for process validation. Establish the required dyne level empirically for the specific adhesive or ink system, then monitor it — nozzle wear, air quality drift and fixture wander all move the result over time.

What to Expect by Substrate

Air plasma raises surface energy on essentially all commodity and engineering polymers, but the size of the gain and the speed of its decay differ enough to change process planning. Indicative behaviour, to be confirmed on the actual part:

Substrate Response to air plasma Decay behaviour
Polypropylene Large gain — among the strongest responses, and the usual reason the equipment was bought Relatively fast; bond within hours where possible
Polyethylene Large gain Fast, and accelerated by slip additive migration
ABS Good gain from an already moderate starting point Moderate
Polycarbonate Good gain; watch for haze at high dose on optical surfaces Moderate
TPE and TPV Good, but oils and plasticisers migrate back quickly Fast — treat immediately before bonding
PPS and high-temperature aromatics Moderate; often already bondable, treatment improves consistency Slow
Silicone and fluoropolymers Limited — these generally need a different route Very fast reversion

Troubleshooting Air Plasma Treatment

Symptom Likely cause Correction
Bond strength varies part to part Standoff distance varying with fixture wear or part presentation Standoff is the most sensitive variable. Fix the fixture before adjusting power — reactive species recombine within millimetres in open air.
Treatment works on a test coupon, fails on the part Line-of-sight shadowing in recesses and undercuts Map which surfaces the head actually reaches. Shadowed geometry points to low-pressure cold gas plasma.
Dyne level good, adhesion poor Contamination reactivated rather than removed, or a weak boundary layer left in place Trace the contaminant — mould release, plasticiser bloom, compressor oil. Air quality to the head must be clean, dry and oil-free.
Result degraded gradually over weeks Nozzle wear, or drift in compressed air quality Put nozzle condition and air dryness on the preventive maintenance schedule, and trend dyne readings rather than spot-checking them.
Surface hazed or visibly damaged Over-treatment — dwell too long or standoff too close Reduce dwell before reducing power. On optical and cosmetic surfaces, qualify the appearance as well as the bond.
Good bond immediately, weak bond next shift Activation decay between treatment and bonding Move the treatment head closer to the bonding station in the process sequence. Treat and bond inline rather than treating in a batch.

Integrating a Head into a Production Cell

Most disappointing air plasma installations are integration problems rather than process problems. The treatment itself is robust; holding it constant is what needs engineering:

  • Treat immediately before bonding. Activation decays over hours to days, so every station between the plasma head and the adhesive is decay time. Inline sequencing beats a treated buffer stock in almost every case.
  • Fix the standoff mechanically. A robot path or a fixed head with a positively located part holds standoff far better than an operator-presented part. This single variable dominates the result.
  • Specify the air. Clean, dry and oil-free is a specification, not an aspiration. Compressor oil carry-over deposits contamination onto the exact surface being cleaned, and it is a common cause of a plant-wide adhesion problem that appears without any process change.
  • Extract the ozone. Local extraction is normally required; confirm the requirement against the plant ventilation assessment.
  • Monitor, do not assume. Wetting tension solutions to ASTM D2578 at the workstation, trended on a chart, will show nozzle wear and air quality drift long before they show up as field failures.
  • Treat only what needs treating. Selective activation of the bond area preserves the appearance and printability of the rest of the part, and reduces the ozone load at the same time.

Related Terms and Reading

Applying this in production

The Sabreen Group provides independent engineering support for electrical air plasma and inline surface activation. If you are specifying a process, qualifying a material or troubleshooting a production problem, our engineering services team can help. Contact us to discuss your application.

Frequently Asked Questions

What is electrical air plasma?

A plasma treatment using ambient air as the working gas, energised by high-voltage electrical discharge to create a reactive plasma field. It modifies surface properties to improve adhesion, without requiring specialty gases or a vacuum environment.

How is the plasma generated?

A strong electrical field — via arc, corona, or dielectric barrier discharge — ionises the ambient air between electrodes or near a nozzle. The ionised air forms a cold reactive plasma containing the species that oxidise and activate the surface.

What can air plasma be used for?

Surface cleaning to remove oils, residues and organic contaminants before coating, painting or bonding; surface activation to raise surface energy for better ink, adhesive and coating adhesion; and micro-etching to lightly roughen the surface for mechanical keying.

How deep does the treatment go?

Not deep. Modifications are superficial, typically confined to the top few nanometres or micrometers of the surface. That is sufficient for adhesion, since bonding is an interfacial phenomenon, but it means the effect is fragile.

Why does treated surface energy fade?

Because polymer chain mobility lets the oxidised functional groups reorient away from the surface, and low molecular weight additives migrate back to it. The effect is time-sensitive, so parts should be bonded or coated quickly after treatment.

Which variable matters most in air plasma treatment?

Standoff distance, by a clear margin. The reactive species that do the work recombine within millimetres in open air, so a few millimetres of variation changes the delivered dose substantially. Fixture repeatability therefore matters more than raw power — if results vary part to part, correct the presentation before adjusting the process settings.

How long after treatment must the part be bonded?

As soon as practical. Activation decays over hours to days as polymer chains reorient and low molecular weight additives migrate back to the surface, and the decay is fastest on polyolefins and on elastomers containing oils or plasticisers. Sequence the plasma head immediately before the bonding or coating station rather than treating into a buffer stock.

Can air plasma treat inside recesses and undercuts?

No — it is a line-of-sight process, so shadowed surfaces receive little or no treatment. This is the most common reason a process that works on a flat test coupon fails on the real moulding. Map which surfaces the head actually reaches; complex internal geometry points towards low-pressure cold gas plasma, which fills the chamber rather than being directed at a surface.


Request your free quote

Scott Sabreen — President and Chief Engineer, with over 30 years of expertise. Contact us today to discuss your application and SABREEN solutions free of charge and with no obligation. Bring us your most difficult challenges.

Phone: +1 972-820-6777

Contact us →

Frequently Asked Questions

What is electrical air plasma treatment?

Electrical air plasma is a corona discharge spot treatment, also called blown air plasma, forced air corona or blown arc. The head carries two hook electrodes close together on a high-voltage transformer, generating an electric arc of roughly 7 to 12 kV at a lower frequency of 50 to 60 cycles per second. Forced air carries the resulting corona discharge onto the part. No positive ground is needed.

How does electrical air plasma differ from electrical corona discharge?

Both are corona discharges, but air plasma runs at a much lower frequency -- 50 to 60 Hz against the 20 to 25 kHz of classical corona discharge -- and needs no earth ground or dielectric barrier. It is a spot treatment rather than an area treatment, which makes it suited to targeted locations rather than to treating a whole surface.

Does electrical air plasma clean the surface?

It has virtually no cleaning capability. Contamination present on the part before treatment will still be there afterwards, so parts carrying mould release, oils or handling residues need cleaning first.

Does corona spot treatment give a longer shelf life than flame treatment?

No -- the opposite, on polyolefins. Scholarly studies show flame plasma produces longer post-treatment shelf life on polyolefins, attributed to its relatively shallower depth of treatment. The belief that corona spot treatment lasts longer is one of the more persistent myths in this area.

Is ozone produced?

Yes. Ozone is generated by the discharge, which needs to be accounted for in the extraction and ventilation design around the treatment station.

Scott Sabreen

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

Describe your problem in two sentences. Scott Sabreen replies personally, usually within one business day.

Submission Successful!

Thank you. Scott has your message and will reply by email, usually within one business day.

We Have Received Your Request

We have received your request and will be in touch shortly.

🌐 India (English) ▴