Surface Pretreatments / Surface Quality - The Sabreen Group, Inc.

Fluorooxidation

Fluorooxidation (F/O) is a surface pretreatment that is conducted inline at ambient conditions. While the science of using Fluorine (F2) gas for surface modification has been well understood for more than 50 years, it has not been widely accepted primarily because of the safety concerns in using Fluorine gas. The significant breakthrough in fluorooxidation as a commercially viable pretreatment for yielding high-strength adhesion bonding is its safe gas processing and eco-friendly neutralization. Small scale, computer-controlled electrolytic cells enable the Fluorine gas to be used safely at low concentrations and low pressures.

An advantage of F/O is its capability to effectively treat large and small surface areas of complex geometry (remote/isolated regions) ranging in size from capillary to large diameter tubes and housings. F/O is an oxidation process, unlike flame and electrical discharge pretreatments which are glow discharge gas phase surface oxidation plasmas. Compared to chamber pressurized RF cold gas plasma treatment, F/O is conducted at ambient conditions. During the F/O processing, a substrate surface is exposed to Fluorine gas and other reactive and non-reactive gases in a controlled chamber. Similar to gas phase surface oxidation processes, oxygen-containing functional groups, such as hydroxyl, carbonyl and carboxyl are created making the surface wettable and very polar. These chemical and physical mechanisms are necessary to achieve strong adhesive bonds.

F/O is used to surface modify ultra-high molecular weight polyethylene (UHMW PE) and high density polyethylene (HDPE) powders to impart a hydrophilic (water-wettable) surface to these normally hydrophobic materials. This change in compatibility, as well as adhesive bonding capability, enables these treated powders to be sold as performance additives for use in polyurethanes, epoxies, rubbers, unsaturated polyesters and even water-borne systems.

F/O treatment is long-lasting and frequently permanent. This is because the treatment chemistry can penetrate considerably deeper than other surface preparation processes. The longevity is important because it avoids the need to use treated items quickly and enables treated substrates to be inventoried for long time periods. Contrary to common belief, use of highly reactive chemicals is actually environmentally friendly. This is because highly reactive chemicals are readily and essentially quantitatively neutralized because they are so reactive. Processes that use unreactive chemicals are some of the most difficult to scrub or neutralize. The spent solid state scrubbing medium used to neutralize the F/O process has commercial value for other manufacturing firms and is sold as a reagent.

Avatar

Scott Sabreen
President & Chief Engineer
30+ Years of Expertise

To arrange a teleconference with Scott Sabreen, please fill out the information below.

What is your mailing address?

Topic of interest?

What industry are you in?

What is the primary plastic type?

Submission Successful!

Your message has been received. We will be in touch shortly to arrange a meeting time.

We Have Received Your Request

We have received your request and will be in touch shortly.